N-LaK9 vs N-LASFN9

Glass · grade comparison

N-LaK9 and N-LASFN9 are both glass grades. N-LaK9 is lighter (3.51 g/cm³ vs 4.44 g/cm³ for N-LASFN9) and N-LaK9 runs hotter in service (500°C vs 400°C continuous). On the shop floor, N-LASFN9 machines more easily (poor vs not recommended).

N-LaK9Choose it when weight is the constraint, or when the part sees heat.

N-LASFN9Choose it when the part is machined in volume.

N-LaK9 vs N-LASFN9: properties

N-LaK9N-LASFN9

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

110 GPa16 Msi
115 GPa16.7 Msi

Shear Modulus

42.7 GPa6.2 Msi
44.7 GPa6.5 Msi

Bulk Modulus

86 GPa12.5 Msi
89 GPa12.9 Msi

Poisson's Ratio

0.29
0.29

Tensile Strength (Ultimate)

55 MPa8 ksi
—

Flexural Strength

70 MPa10.2 ksi
60 MPa8.7 ksi

Fracture Toughness (K_IC)

0.8 MPa·√m0.73 ksi·√in
0.85 MPa·√m0.77 ksi·√in

Hardness, Vickers

640 HV
620 HV

Hardness, Knoop

680 HK
640 HK

Same in both: Compressive Strength 1,000 MPa145 ksi · Hardness, Mohs 6

Physical

Density and transition temperatures.

Density

3.51 g/cm³0.13 lb/in³
4.44 g/cm³0.16 lb/in³

Refractive Index

1.691
1.85

Light Transmission

100%
100%

Same in both: Porosity 0%

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.9 W/m·K0.52 BTU/hr·ft·°F
0.79 W/m·K0.46 BTU/hr·ft·°F

Specific Heat Capacity

510 J/kg·K0.12 BTU/lb·°F
450 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

6.3 µm/m·K3.5 µin/in·°F
7.4 µm/m·K4.1 µin/in·°F

Max Service Temperature (continuous)

500°C932 °F
400°C752 °F

Min Service Temperature

-60°C-76 °F
-100°C-148 °F

Electrical

Conductivity and insulation.

Dielectric Constant (1 MHz)

8.5
—

Volume Resistivity

1×10¹⁴ Ω·cm
—

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

62 / 100
72 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

12 / 100
30 / 100

Polishability

85 / 100
82 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

60 MJ/kg25,795 BTU/lb
90 MJ/kg38,693 BTU/lb

Embodied Carbon (primary production)

4.5 kg CO₂/kg
7 kg CO₂/kg

Embodied Water

120 L/kg14.4 gal/lb
60 L/kg7.2 gal/lb

Typical Recycled Content

20%
3%

Common Calculations

Ratios derived from the values above.

Specific Stiffness (E / density)

31.3 MN·m/kg
25.9 MN·m/kg

Thermal Diffusivity

0.5 mm²/s
0.4 mm²/s

Strength versus weight

Yield strength against density for every glass grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005002.533.5Density (g/cm³)Yield strength (MPa) — log scale

Manufacturing and finishing

CapabilityN-LaK9N-LASFN9
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

N-LaK9 vs N-LASFN9 — frequently asked

What is the difference between N-LaK9 and N-LASFN9?

N-LaK9 and N-LASFN9 are both glass grades. N-LaK9 is lighter (3.51 g/cm³ vs 4.44 g/cm³ for N-LASFN9) and N-LaK9 runs hotter in service (500°C vs 400°C continuous). On the shop floor, N-LASFN9 machines more easily (poor vs not recommended).

Which is cheaper, N-LaK9 or N-LASFN9?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which is easier to machine, N-LaK9 or N-LASFN9?

N-LASFN9. Its machinability rates poor (30/100) against not recommended (12/100) for N-LaK9.

Ready to make it?

Upload a CAD file and FabDigit prices the part in N-LaK9 and N-LASFN9 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.