CC753S-GC and CC753S-GM are two conditions of the same copper alloy grade, CC753S: GC (continuously cast bar/tube) versus GM (permanent (gravity die) cast). The chemistry is identical, so every difference below comes from the condition. CC753S-GC is the stronger of the two: yield strength 200 MPa (29 ksi) against 180 MPa (26.1 ksi) for CC753S-GM, about 11% more; tensile strength follows at 390 MPa (56.6 ksi) vs 360 MPa (52.2 ksi). CC753S-GC is harder — 95 HB against 90 HB for CC753S-GM — which matters for wear surfaces and threads.

CC753S-GCChoose it when strength drives the design, or when surface hardness matters.

CC753S-GC vs CC753S-GM: properties

CC753S-GCCC753S-GM

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

100 GPa14.5 Msi
97 GPa14.1 Msi

Tensile Strength (Ultimate)

390 MPa56.6 ksi
360 MPa52.2 ksi

Yield Strength (0.2% offset)

200 MPa29 ksi
180 MPa26.1 ksi

Reduction in Area

20%
18%

Compressive Strength

390 MPa56.6 ksi
360 MPa52.2 ksi

Shear Strength

265 MPa38.4 ksi
250 MPa36.3 ksi

Fatigue Strength (Endurance Limit)

110 MPa16 ksi
100 MPa14.5 ksi

Charpy V-Notch Impact (RT)

20 J14.8 ft·lbf
18 J13.3 ft·lbf

Hardness, Brinell

95 HB
90 HB

Hardness, Rockwell B

56 HRB
52 HRB

Hardness, Vickers

100 HV
95 HV

Same in both: Shear Modulus 36 GPa5.2 Msi · Bulk Modulus 110 GPa16 Msi · Poisson's Ratio 0.34 · Elongation at Break 15%

Physical

Density and transition temperatures.

Same in both: Density 8.4 g/cm³0.3 lb/in³ · Melting Point (Solidus) 880°C1,616 °F · Liquidus Temperature 905°C1,661 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

100 W/m·K57.8 BTU/hr·ft·°F
98 W/m·K56.6 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 377 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 21 µm/m·K11.7 µin/in·°F · Latent Heat of Fusion 170 J/g73.1 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -100°C-148 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

20 % IACS
19 % IACS

Electrical Resistivity

8.6×10⁻⁸ Ω·m3.39 µΩ·in
9.1×10⁻⁸ Ω·m3.58 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

58 / 100
57 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.28 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

82 / 100
78 / 100

Machinability Rating (AISI 1212 = 100 %)

72%
68%

Formability (cold)

18 / 100
15 / 100

Same in both: Weldability 25 / 100 · Castability 80 / 100 · Brazeability / Solderability 55 / 100 · Polishability 65 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 55 MJ/kg23,646 BTU/lb · Embodied Carbon (primary production) 3.6 kg CO₂/kg · Embodied Water 260 L/kg31.2 gal/lb · Typical Recycled Content 80%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleCC753S

CC753S-GC vs CC753S-GM — frequently asked

Is CC753S-GC stronger than CC753S-GM?

Yes. CC753S-GC has a typical yield strength of 200 MPa (29 ksi) against 180 MPa (26.1 ksi) for CC753S-GM — about 11% more. Tensile strength is 390 MPa (56.6 ksi) vs 360 MPa (52.2 ksi).

Which condition does FabDigit quote by default, GC or GM?

GS is the default CC753S condition in the FabDigit quote flow (neither GC nor GM). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose CC753S-GC over CC753S-GM?

Pick CC753S-GC when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in CC753S-GC and CC753S-GM side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.