Copper Alloy CC498K-GM vs CC498K-GZ

Copper Alloy · CC498K temper comparison

CC498K-GM and CC498K-GZ are two conditions of the same copper alloy grade, CC498K: GM (permanent (chill) mould cast) versus GZ (centrifugally cast). The chemistry is identical, so every difference below comes from the condition. CC498K-GZ is the stronger of the two: yield strength 140 MPa (20.3 ksi) against 130 MPa (18.9 ksi) for CC498K-GM, about 8% more. CC498K-GZ is harder — 38 HRB against 35 HRB for CC498K-GM — which matters for wear surfaces and threads.

CC498K-GZChoose it when strength drives the design, or when surface hardness matters.

CC498K-GM vs CC498K-GZ: properties

CC498K-GMCC498K-GZ

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

92 GPa13.3 Msi
95 GPa13.8 Msi

Tensile Strength (Ultimate)

260 MPa37.7 ksi
270 MPa39.2 ksi

Yield Strength (0.2% offset)

130 MPa18.9 ksi
140 MPa20.3 ksi

Shear Strength

195 MPa28.3 ksi
200 MPa29 ksi

Fatigue Strength (Endurance Limit)

88 MPa12.8 ksi
92 MPa13.3 ksi

Charpy V-Notch Impact (RT)

19 J14 ft·lbf
18 J13.3 ft·lbf

Hardness, Brinell

72 HB
75 HB

Hardness, Rockwell B

35 HRB
38 HRB

Hardness, Vickers

76 HV
79 HV

Same in both: Shear Modulus 36 GPa5.2 Msi · Bulk Modulus 105 GPa15.2 Msi · Poisson's Ratio 0.34 · Elongation at Break 13% · Reduction in Area 13%

Physical

Density and transition temperatures.

Same in both: Density 8.8 g/cm³0.32 lb/in³ · Melting Point (Solidus) 855°C1,571 °F · Liquidus Temperature 1,000°C1,832 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 60 W/m·K34.7 BTU/hr·ft·°F · Specific Heat Capacity 380 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 18.5 µm/m·K10.3 µin/in·°F · Latent Heat of Fusion 170 J/g73.1 BTU/lb · Max Service Temperature (continuous) 250°C482 °F · Min Service Temperature -200°C-328 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 12 % IACS · Electrical Resistivity 1.44×10⁻⁷ Ω·m5.67 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

65 / 100
66 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.25 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Same in both: Machinability 80 / 100 · Machinability Rating (AISI 1212 = 100 %) 80% · Weldability 30 / 100 · Formability (cold) 10 / 100 · Castability 85 / 100 · Brazeability / Solderability 70 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 50 MJ/kg21,496 BTU/lb · Embodied Carbon (primary production) 3.5 kg CO₂/kg · Embodied Water 250 L/kg30 gal/lb · Typical Recycled Content 60%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleCC498K

CC498K-GM vs CC498K-GZ — frequently asked

Is CC498K-GZ stronger than CC498K-GM?

Yes. CC498K-GZ has a typical yield strength of 140 MPa (20.3 ksi) against 130 MPa (18.9 ksi) for CC498K-GM — about 8% more. Tensile strength is 270 MPa (39.2 ksi) vs 260 MPa (37.7 ksi).

Which condition does FabDigit quote by default, GM or GZ?

GC is the default CC498K condition in the FabDigit quote flow (neither GM nor GZ). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose CC498K-GM over CC498K-GZ?

Pick CC498K-GZ when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in CC498K-GM and CC498K-GZ side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.