FabDigitFabDigit

Copper Alloy CC491K-GC vs CC491K-GZ

Copper Alloy · CC491K temper comparison

CC491K-GC and CC491K-GZ are two conditions of the same copper alloy grade, CC491K: GC (continuously cast bar/tube) versus GZ (centrifugally cast). The chemistry is identical, so every difference below comes from the condition. CC491K-GC is the stronger of the two: yield strength 140 MPa (20.3 ksi) against 130 MPa (18.9 ksi) for CC491K-GZ, about 8% more. CC491K-GC is harder — 70 HB against 65 HB for CC491K-GZ — which matters for wear surfaces and threads.

CC491K-GCChoose it when strength drives the design, or when surface hardness matters.

CC491K-GC vs CC491K-GZ: properties

CC491K-GCCC491K-GZ

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

103 GPa14.9 Msi
102 GPa14.8 Msi

Tensile Strength (Ultimate)

275 MPa39.9 ksi
270 MPa39.2 ksi

Yield Strength (0.2% offset)

140 MPa20.3 ksi
130 MPa18.9 ksi

Elongation at Break

15%
14%

Reduction in Area

18%
17%

Compressive Strength

275 MPa39.9 ksi
265 MPa38.4 ksi

Hardness, Brinell

70 HB
65 HB

Hardness, Rockwell B

40 HRB
35 HRB

Hardness, Vickers

73 HV
68 HV

Same in both: Shear Modulus 37 GPa5.4 Msi · Bulk Modulus 104 GPa15.1 Msi · Poisson's Ratio 0.34 · Shear Strength 200 MPa29 ksi · Fatigue Strength (Endurance Limit) 85 MPa12.3 ksi · Charpy V-Notch Impact (RT) 12 J8.9 ft·lbf

Physical

Density and transition temperatures.

Same in both: Density 8.83 g/cm³0.32 lb/in³ · Melting Point (Solidus) 854°C1,569 °F · Liquidus Temperature 1,010°C1,850 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 72 W/m·K41.6 BTU/hr·ft·°F · Specific Heat Capacity 377 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 18 µm/m·K10 µin/in·°F · Latent Heat of Fusion 170 J/g73.1 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 15 % IACS · Electrical Resistivity 1.15×10⁻⁷ Ω·m4.53 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

73 / 100
72 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.25 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

87 / 100
85 / 100

Same in both: Machinability Rating (AISI 1212 = 100 %) 84% · Weldability 25 / 100 · Formability (cold) 15 / 100 · Castability 90 / 100 · Brazeability / Solderability 75 / 100 · Polishability 65 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 52 MJ/kg22,356 BTU/lb · Embodied Carbon (primary production) 3.6 kg CO₂/kg · Embodied Water 250 L/kg30 gal/lb · Typical Recycled Content 80%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleCC491K

CC491K-GC vs CC491K-GZ — frequently asked

Is CC491K-GC stronger than CC491K-GZ?

Yes. CC491K-GC has a typical yield strength of 140 MPa (20.3 ksi) against 130 MPa (18.9 ksi) for CC491K-GZ — about 8% more. Tensile strength is 275 MPa (39.9 ksi) vs 270 MPa (39.2 ksi).

Which condition does FabDigit quote by default, GC or GZ?

GS is the default CC491K condition in the FabDigit quote flow (neither GC nor GZ). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose CC491K-GC over CC491K-GZ?

Pick CC491K-GC when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in CC491K-GC and CC491K-GZ side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.