G-9 vs XXXP
Composite · grade comparison
G-9 and XXXP are both composite grades. G-9 is the stronger of the two: tensile strength 240 MPa (34.8 ksi) against 105 MPa (15.2 ksi) for XXXP, about 129% more. XXXP is lighter (1.35 g/cm³ vs 1.95 g/cm³ for G-9) and G-9 is stiffer (19 GPa vs 9 GPa). On the shop floor, XXXP machines more easily (excellent vs poor) and XXXP sits in a lower cost tier (standard, $$) than G-9 (high, $$$$).
G-9Choose it when strength drives the design, or when the part sees heat.
XXXPChoose it when weight is the constraint, or when the part is machined in volume.
G-9 vs XXXP: propertiesHow to read these bars
- One bar per material. A full bar is the highest value among all composite grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
How to read these bars
- One bar per material. A full bar is the highest value among all composite grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
Mechanical
Strength, stiffness, ductility and hardness at room temperature.
Elastic (Young's) Modulus
Poisson's Ratio
Tensile Strength (Ultimate)
Compressive Strength
Compressive Modulus
Flexural Strength
Flexural Modulus
Shear Strength
Izod Impact, Notched
Hardness, Rockwell M
Elongation at Break
Physical
Density and transition temperatures.
Density
Water Absorption (24 h)
Water Absorption (Saturation)
Glass Transition (Tg)
Thermal
How each material carries heat and how hot it can run.
Thermal Conductivity
Specific Heat Capacity
Thermal Expansion (CTE, 20–100 °C)
Max Service Temperature (continuous)
Min Service Temperature
Limiting Oxygen Index
Max Service Temperature (short-term)
Electrical
Conductivity and insulation.
Electrical Resistivity
Dielectric Strength
Dielectric Constant (1 MHz)
Dissipation Factor (1 MHz)
Volume Resistivity
Comparative Tracking Index (CTI)
Same in both: Surface Resistivity 1×10¹² Ω
Chemical & Environmental
Corrosion and environmental resistance (0–100 scores).
Corrosion Resistance
UV / Weathering Resistance
Manufacturability
FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.
Machinability
Polishability
Sustainability
Primary-production footprint per kilogram.
Embodied Energy (primary production)
Embodied Carbon (primary production)
Embodied Water
Same in both: Typical Recycled Content 0%
Common Calculations
Ratios derived from the values above.
Specific Strength (UTS / density)
Specific Stiffness (E / density)
Same in both: Thermal Diffusivity 0.1 mm²/s · Thermal Shock Resistance Index 0
Strength versus weight
Yield strength against density for every composite grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.
Manufacturing and finishing
| Capability | G-9 | XXXP |
|---|---|---|
| Default condition | — | — |
| Relative cost | $$$$ High | $$ Standard |
| Min. machined wall | — | — |
| Best machined surface | — | — |
G-9 vs XXXP — frequently asked
Is G-9 stronger than XXXP?
Yes. G-9 has a typical tensile strength of 240 MPa (34.8 ksi) against 105 MPa (15.2 ksi) for XXXP — about 129% more.
Which is cheaper, G-9 or XXXP?
XXXP is the lower-cost material: it sits in the standard tier ($$) while G-9 is high ($$$$). Part price depends far more on geometry, tolerance and quantity than on raw stock — upload a CAD file for a live quote.
Which is easier to machine, G-9 or XXXP?
XXXP. Its machinability rates excellent (85/100) against poor (30/100) for G-9.
Ready to make it?
Upload a CAD file and FabDigit prices the part in G-9 and XXXP side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.
Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.