FR-6 vs GPO-2
Composite · grade comparison
FR-6 and GPO-2 are both composite grades. GPO-2 is stiffer (11 GPa vs 10 GPa).
FR-6 vs GPO-2: propertiesHow to read these bars
- One bar per material. A full bar is the highest value among all composite grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
How to read these bars
- One bar per material. A full bar is the highest value among all composite grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
Mechanical
Strength, stiffness, ductility and hardness at room temperature.
Elastic (Young's) Modulus
Shear Modulus
Poisson's Ratio
Elongation at Break
Compressive Strength
Compressive Modulus
Flexural Strength
Flexural Modulus
Shear Strength
Izod Impact, Notched
Same in both: Tensile Strength (Ultimate) 85 MPa12.3 ksi · Hardness, Rockwell M 105 HRM
Physical
Density and transition temperatures.
Water Absorption (24 h)
Water Absorption (Saturation)
Same in both: Density 1.85 g/cm³0.07 lb/in³ · Glass Transition (Tg) 120°C248 °F
Thermal
How each material carries heat and how hot it can run.
Thermal Conductivity
Specific Heat Capacity
Thermal Expansion (CTE, 20–100 °C)
Max Service Temperature (continuous)
Heat Deflection Temp. @ 1.8 MPa
Same in both: Min Service Temperature -40°C-40 °F · Limiting Oxygen Index 32% · Max Service Temperature (short-term) 180°C356 °F
Electrical
Conductivity and insulation.
Electrical Resistivity
Dielectric Constant (1 MHz)
Dissipation Factor (1 MHz)
Volume Resistivity
Surface Resistivity
Comparative Tracking Index (CTI)
Same in both: Dielectric Strength 14 kV/mm356 V/mil
Chemical & Environmental
Corrosion and environmental resistance (0–100 scores).
Corrosion Resistance
Same in both: UV / Weathering Resistance 45 / 100
Manufacturability
FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.
Machinability
Same in both: Polishability 20 / 100
Sustainability
Primary-production footprint per kilogram.
Embodied Energy (primary production)
Embodied Carbon (primary production)
Embodied Water
Same in both: Typical Recycled Content 0%
Common Calculations
Ratios derived from the values above.
Specific Stiffness (E / density)
Thermal Diffusivity
Same in both: Specific Strength (UTS / density) 46 kN·m/kg · Thermal Shock Resistance Index 0
Strength versus weight
Yield strength against density for every composite grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.
Manufacturing and finishing
| Capability | FR-6 | GPO-2 |
|---|---|---|
| Default condition | — | — |
| Relative cost | $$$ Premium | $$$ Premium |
| Min. machined wall | — | — |
| Best machined surface | — | — |
FR-6 vs GPO-2 — frequently asked
What is the difference between FR-6 and GPO-2?
FR-6 and GPO-2 are both composite grades. GPO-2 is stiffer (11 GPa vs 10 GPa).
Which is cheaper, FR-6 or GPO-2?
Both sit in the same relative cost tier ($$$, premium); the part price will be decided by machining time, tolerance and quantity rather than by the material.
Which is easier to machine, FR-6 or GPO-2?
FR-6, by a small margin. Both rate fair for machinability — 45/100 against 38/100 for GPO-2.
Ready to make it?
Upload a CAD file and FabDigit prices the part in FR-6 and GPO-2 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.
Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.