FabDigit

SUM43 vs 1117 and 2 more: properties

SUM43111711411215

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

205 GPa29.7 Msi
200 GPa29 Msi
200 GPa29 Msi
200 GPa29 Msi

Tensile Strength (Ultimate)

700 MPa102 ksi
425 MPa61.6 ksi
675 MPa97.9 ksi
415 MPa60.2 ksi

Yield Strength (0.2% offset)

620 MPa89.9 ksi
235 MPa34.1 ksi
360 MPa52.2 ksi
250 MPa36.3 ksi

Elongation at Break

10%
33%
22%
25%

Reduction in Area

25%
58%
38%
45%

Compressive Strength

620 MPa89.9 ksi

Shear Strength

420 MPa60.9 ksi
320 MPa46.4 ksi
405 MPa58.7 ksi
290 MPa42.1 ksi

Fatigue Strength (Endurance Limit)

310 MPa45 ksi
200 MPa29 ksi
300 MPa43.5 ksi
190 MPa27.6 ksi

Fracture Toughness (K_IC)

50 MPa·√m45.5 ksi·√in

Charpy V-Notch Impact (RT)

14 J10.3 ft·lbf
50 J36.9 ft·lbf
30 J22.1 ft·lbf

Hardness, Brinell

212 HB
121 HB
192 HB
121 HB

Hardness, Rockwell B

95 HRB
68 HRB
92 HRB
70 HRB

Same in both: Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Density

7.85 g/cm³0.28 lb/in³
7.87 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.87 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,420°C2,588 °F
1,420°C2,588 °F
1,425°C2,597 °F
1,420°C2,588 °F

Liquidus Temperature

1,490°C2,714 °F
1,500°C2,732 °F
1,490°C2,714 °F
1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

48 W/m·K27.7 BTU/hr·ft·°F
51 W/m·K29.5 BTU/hr·ft·°F
49 W/m·K28.3 BTU/hr·ft·°F
51.9 W/m·K30 BTU/hr·ft·°F

Specific Heat Capacity

480 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
486 J/kg·K0.12 BTU/lb·°F
486 J/kg·K0.12 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.5 µm/m·K6.4 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F

Latent Heat of Fusion

260 J/g112 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb
247 J/g106 BTU/lb

Max Service Temperature (continuous)

300°C572 °F
400°C752 °F
425°C797 °F
400°C752 °F

Same in both: Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

9.5 % IACS
10.8 % IACS
9.5 % IACS
10.8 % IACS

Electrical Resistivity

1.8×10⁻⁷ Ω·m7.09 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in
1.8×10⁻⁷ Ω·m7.09 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.61 V
-0.61 V
-0.61 V

Corrosion Resistance

10 / 100
10 / 100
10 / 100
8 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

80 / 100
70 / 100
68 / 100
85 / 100

Machinability Rating (AISI 1212 = 100 %)

80%
91%
70%
120%

Weldability

20 / 100
50 / 100
25 / 100
20 / 100

Formability (cold)

25 / 100
60 / 100
35 / 100
35 / 100

Brazeability / Solderability

55 / 100
65 / 100
55 / 100
55 / 100

Polishability

55 / 100
45 / 100
55 / 100
40 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb
26 MJ/kg11,178 BTU/lb

Embodied Carbon (primary production)

1.9 kg CO₂/kg
1.9 kg CO₂/kg
1.9 kg CO₂/kg
2 kg CO₂/kg

Embodied Water

40 L/kg4.8 gal/lb
45 L/kg5.4 gal/lb
45 L/kg5.4 gal/lb
45 L/kg5.4 gal/lb

Typical Recycled Content

30%
30%
30%
35%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

89 kN·m/kg
54 kN·m/kg
86 kN·m/kg
53 kN·m/kg

Specific Stiffness (E / density)

26.1 MN·m/kg
25.4 MN·m/kg
25.5 MN·m/kg
25.4 MN·m/kg

Modulus of Resilience

938 kJ/m³
138 kJ/m³
324 kJ/m³
156 kJ/m³

Thermal Diffusivity

12.7 mm²/s
13.8 mm²/s
12.8 mm²/s
13.6 mm²/s

Thermal Shock Resistance Index

14
9
14
9

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale111711411215SUM43

Manufacturing and finishing

CapabilitySUM43111711411215
CNC machiningYesYesYes
Default conditionHRHRHR
Relative cost$ Budget$ Budget$$ Standard$ Budget
Min. machined wall0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µm
AlCrNYesYesYes
AlTiNYesYesYes
Black OxideYesYesYes
CVD Al2O3YesYesYes
CVD TiCNYesYesYes
CVD TiNYesYesYes
CerakoteYesYesYes
Chrome PlatingYesYesYes
CrNYesYesYes
DLCYesYesYes
E-CoatingYesYesYes
HVOF CoatingYesYesYes
Hot-Dip GalvanizingYesYesYes
MoS2YesYesYes
Multilayer CVDYesYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SUM43 and 1117 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.