FabDigit

SECC vs A588 and 2 more: properties

SECCA588A653SGCC

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

205 GPa29.7 Msi
200 GPa29 Msi
200 GPa29 Msi
205 GPa29.7 Msi

Shear Modulus

80 GPa11.6 Msi
79 GPa11.5 Msi
79 GPa11.5 Msi
80 GPa11.6 Msi

Tensile Strength (Ultimate)

340 MPa49.3 ksi
520 MPa75.4 ksi
360 MPa52.2 ksi
330 MPa47.9 ksi

Yield Strength (0.2% offset)

240 MPa34.8 ksi
380 MPa55.1 ksi
260 MPa37.7 ksi
250 MPa36.3 ksi

Elongation at Break

36%
25%
32%
33%

Reduction in Area

62%
45%
55%
60%

Compressive Strength

245 MPa35.5 ksi
380 MPa55.1 ksi
260 MPa37.7 ksi
250 MPa36.3 ksi

Shear Strength

230 MPa33.4 ksi
320 MPa46.4 ksi
235 MPa34.1 ksi
235 MPa34.1 ksi

Fatigue Strength (Endurance Limit)

170 MPa24.7 ksi
240 MPa34.8 ksi
170 MPa24.7 ksi
165 MPa23.9 ksi

Fracture Toughness (K_IC)

140 MPa·√m127 ksi·√in
120 MPa·√m109 ksi·√in
100 MPa·√m91 ksi·√in

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
60 J44.3 ft·lbf
35 J25.8 ft·lbf
55 J40.6 ft·lbf

Hardness, Brinell

105 HB
155 HB
110 HB
102 HB

Hardness, Rockwell B

58 HRB
83 HRB
62 HRB
58 HRB

Hardness, Vickers

112 HV
163 HV
115 HV
110 HV

Same in both: Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,500°C2,732 °F
1,490°C2,714 °F
1,495°C2,723 °F
1,500°C2,732 °F

Liquidus Temperature

1,528°C2,782 °F
1,520°C2,768 °F
1,520°C2,768 °F
1,530°C2,786 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Specific Heat Capacity

480 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12 µm/m·K6.7 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
12 µm/m·K6.7 µin/in·°F
12 µm/m·K6.7 µin/in·°F

Latent Heat of Fusion

270 J/g116 BTU/lb
250 J/g107 BTU/lb
270 J/g116 BTU/lb
270 J/g116 BTU/lb

Max Service Temperature (continuous)

400°C752 °F
400°C752 °F
200°C392 °F
400°C752 °F

Min Service Temperature

-40°C-40 °F
-40°C-40 °F
-30°C-22 °F
-30°C-22 °F

Same in both: Thermal Conductivity 52 W/m·K30 BTU/hr·ft·°F

Electrical

Conductivity and insulation.

Electrical Conductivity

11 % IACS
8.6 % IACS
10.5 % IACS
10.5 % IACS

Electrical Resistivity

1.6×10⁻⁷ Ω·m6.3 µΩ·in
2×10⁻⁷ Ω·m7.87 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.98 V
-0.65 V
-1.02 V
-1.03 V

Corrosion Resistance

8 / 100
32 / 100
38 / 100
10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
55 / 100
62 / 100
68 / 100

Machinability Rating (AISI 1212 = 100 %)

55%
58%
66%
68%

Weldability

88 / 100
78 / 100
72 / 100
88 / 100

Formability (cold)

75 / 100
60 / 100
82 / 100
72 / 100

Brazeability / Solderability

70 / 100
55 / 100
70 / 100
60 / 100

Polishability

35 / 100
45 / 100
25 / 100
30 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

35 MJ/kg15,047 BTU/lb
25 MJ/kg10,748 BTU/lb
30 MJ/kg12,898 BTU/lb
32 MJ/kg13,758 BTU/lb

Embodied Carbon (primary production)

2.5 kg CO₂/kg
2 kg CO₂/kg
2.5 kg CO₂/kg
2.4 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
45 L/kg5.4 gal/lb
60 L/kg7.2 gal/lb
45 L/kg5.4 gal/lb

Typical Recycled Content

25%
30%
30%
25%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

43 kN·m/kg
66 kN·m/kg
46 kN·m/kg
42 kN·m/kg

Specific Stiffness (E / density)

26.1 MN·m/kg
25.5 MN·m/kg
25.5 MN·m/kg
26.1 MN·m/kg

Modulus of Resilience

140 kJ/m³
361 kJ/m³
169 kJ/m³
152 kJ/m³

Thermal Diffusivity

13.8 mm²/s
14.4 mm²/s
14.1 mm²/s
13.9 mm²/s

Thermal Shock Resistance Index

7
12
8
7

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleA588A653SECCSGCC

Manufacturing and finishing

CapabilitySECCA588A653SGCC
CNC machiningYes
Default conditionHRHRHRHR
Relative cost$$ Standard$$ Standard$$ Standard$$ Standard
Min. machined wall0.8 mm
Best machined surfaceRa 1.6 µm
AlCrNYes
AlTiNYes
CVD Al2O3Yes
CVD TiCNYes
CVD TiNYes
CrNYes
DLCYes
HVOF CoatingYes
MoS2Yes
Multilayer CVDYes
TiAlNYes
TiB2Yes
TiCNYes
TiNYes
WC/CYes
ZrNYes

Both are offered for Sheet metal. They share 22 finishes: Black Oxide, Cerakote, Chrome Plating, Copper Plating, E-Coating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Hot-Dip Galvanizing, Manganese Phosphate, Nickel Plating and 10 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SECC and A588 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.