SCM418SCM41543204620

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

205 GPa29.7 Msi
206 GPa29.9 Msi
205 GPa29.7 Msi
205 GPa29.7 Msi

Tensile Strength (Ultimate)

560 MPa81.2 ksi
640 MPa92.8 ksi
640 MPa92.8 ksi
570 MPa82.7 ksi

Yield Strength (0.2% offset)

355 MPa51.5 ksi
430 MPa62.4 ksi
415 MPa60.2 ksi
360 MPa52.2 ksi

Elongation at Break

26%
22%
22%
26%

Reduction in Area

57%
55%
50%
55%

Compressive Strength

360 MPa52.2 ksi
430 MPa62.4 ksi

Shear Strength

380 MPa55.1 ksi
400 MPa58 ksi
415 MPa60.2 ksi
380 MPa55.1 ksi

Fatigue Strength (Endurance Limit)

260 MPa37.7 ksi
290 MPa42.1 ksi
300 MPa43.5 ksi
260 MPa37.7 ksi

Fracture Toughness (K_IC)

90 MPa·√m81.9 ksi·√in
90 MPa·√m81.9 ksi·√in

Charpy V-Notch Impact (RT)

90 J66.4 ft·lbf
55 J40.6 ft·lbf
70 J51.6 ft·lbf
85 J62.7 ft·lbf

Hardness, Brinell

163 HB
180 HB
187 HB
163 HB

Hardness, Rockwell B

84 HRB
89 HRB
90 HRB
84 HRB

Hardness, Vickers

171 HV
190 HV

Same in both: Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,420°C2,588 °F
1,430°C2,606 °F
1,425°C2,597 °F
1,420°C2,588 °F

Liquidus Temperature

1,500°C2,732 °F
1,510°C2,750 °F
1,500°C2,732 °F
1,500°C2,732 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

42 W/m·K24.3 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F
46 W/m·K26.6 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
473 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12.3 µm/m·K6.8 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
250 J/g107 BTU/lb
270 J/g116 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

200°C392 °F
400°C752 °F
350°C662 °F
400°C752 °F

Min Service Temperature

-40°C-40 °F
-50°C-58 °F
-60°C-76 °F
-50°C-58 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

7.8 % IACS
7.8 % IACS
8 % IACS

Same in both: Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.61 V
-0.61 V
-0.6 V
-0.61 V

Corrosion Resistance

12 / 100
12 / 100
11 / 100
12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
58 / 100
50 / 100
57 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
60%
55%
65%

Weldability

55 / 100
55 / 100
40 / 100
65 / 100

Formability (cold)

58 / 100
60 / 100
45 / 100
58 / 100

Brazeability / Solderability

65 / 100
65 / 100
55 / 100
70 / 100

Polishability

60 / 100
60 / 100
60 / 100
55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

30 MJ/kg12,898 BTU/lb
27 MJ/kg11,608 BTU/lb
31 MJ/kg13,328 BTU/lb
29 MJ/kg12,468 BTU/lb

Embodied Carbon (primary production)

2.2 kg CO₂/kg
2.1 kg CO₂/kg
2.3 kg CO₂/kg
2.2 kg CO₂/kg

Embodied Water

45 L/kg5.4 gal/lb
50 L/kg6 gal/lb
50 L/kg6 gal/lb
55 L/kg6.6 gal/lb

Same in both: Typical Recycled Content 30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

71 kN·m/kg
82 kN·m/kg
82 kN·m/kg
73 kN·m/kg

Specific Stiffness (E / density)

26.1 MN·m/kg
26.2 MN·m/kg
26.1 MN·m/kg
26.1 MN·m/kg

Modulus of Resilience

307 kJ/m³
449 kJ/m³
420 kJ/m³
316 kJ/m³

Thermal Diffusivity

11.4 mm²/s
11.9 mm²/s
11.8 mm²/s
12.3 mm²/s

Thermal Shock Resistance Index

9
11
12
11

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSCM41543204620SCM418

Manufacturing and finishing

CapabilitySCM418SCM41543204620
CNC machiningYesYesYes
Sheet metalYesYesYes
Default conditionHRHRHR
Relative cost$ Budget$$ Standard$$$ Premium$$ Standard
Min. machined wall0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µm
AlCrNYesYesYes
AlTiNYesYesYes
Black OxideYesYesYes
CVD Al2O3YesYesYes
CVD TiCNYesYesYes
CVD TiNYesYesYes
CerakoteYesYesYes
Chrome PlatingYesYesYes
CrNYesYesYes
DLCYesYesYes
E-CoatingYesYesYes
HVOF CoatingYesYesYes
Hot-Dip GalvanizingYesYesYes
MoS2YesYesYes
Multilayer CVDYesYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SCM418 and SCM415 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.