FabDigit

E355 vs 1030 and 2 more: properties

E355103010351040

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

210 GPa30.5 Msi
205 GPa29.7 Msi
205 GPa29.7 Msi
205 GPa29.7 Msi

Tensile Strength (Ultimate)

650 MPa94.3 ksi
470 MPa68.2 ksi
585 MPa84.8 ksi
620 MPa89.9 ksi

Yield Strength (0.2% offset)

490 MPa71.1 ksi
260 MPa37.7 ksi
320 MPa46.4 ksi
415 MPa60.2 ksi

Elongation at Break

10%
20%
18%
25%

Reduction in Area

45%
42%
40%
50%

Compressive Strength

490 MPa71.1 ksi
260 MPa37.7 ksi
320 MPa46.4 ksi
415 MPa60.2 ksi

Shear Strength

390 MPa56.6 ksi
300 MPa43.5 ksi
360 MPa52.2 ksi
385 MPa55.8 ksi

Fatigue Strength (Endurance Limit)

290 MPa42.1 ksi
230 MPa33.4 ksi
260 MPa37.7 ksi
290 MPa42.1 ksi

Fracture Toughness (K_IC)

60 MPa·√m54.6 ksi·√in
55 MPa·√m50.1 ksi·√in
60 MPa·√m54.6 ksi·√in
55 MPa·√m50.1 ksi·√in

Charpy V-Notch Impact (RT)

30 J22.1 ft·lbf
40 J29.5 ft·lbf
55 J40.6 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

190 HB
137 HB
163 HB
201 HB

Hardness, Rockwell B

92 HRB
75 HRB
85 HRB
93 HRB

Hardness, Vickers

200 HV
170 HV
210 HV

Same in both: Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,460°C2,660 °F
1,425°C2,597 °F
1,425°C2,597 °F
1,425°C2,597 °F

Liquidus Temperature

1,520°C2,768 °F
1,510°C2,750 °F
1,500°C2,732 °F
1,495°C2,723 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

45 W/m·K26 BTU/hr·ft·°F
51.9 W/m·K30 BTU/hr·ft·°F
49 W/m·K28.3 BTU/hr·ft·°F
51 W/m·K29.5 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
486 J/kg·K0.12 BTU/lb·°F
486 J/kg·K0.12 BTU/lb·°F
486 J/kg·K0.12 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12 µm/m·K6.7 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F
11.5 µm/m·K6.4 µin/in·°F

Latent Heat of Fusion

270 J/g116 BTU/lb
247 J/g106 BTU/lb
250 J/g107 BTU/lb
247 J/g106 BTU/lb

Max Service Temperature (continuous)

350°C662 °F
400°C752 °F
425°C797 °F
425°C797 °F

Same in both: Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

8.6 % IACS
10 % IACS
10.8 % IACS
10 % IACS

Electrical Resistivity

2×10⁻⁷ Ω·m7.87 µΩ·in
1.7×10⁻⁷ Ω·m6.69 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in
1.71×10⁻⁷ Ω·m6.73 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

58 / 100
55 / 100
60 / 100
55 / 100

Machinability Rating (AISI 1212 = 100 %)

62%
65%
65%
60%

Weldability

72 / 100
62 / 100
55 / 100
45 / 100

Formability (cold)

40 / 100
50 / 100
50 / 100
45 / 100

Brazeability / Solderability

60 / 100
70 / 100
65 / 100
60 / 100

Polishability

55 / 100
55 / 100
60 / 100
60 / 100

Castability

45 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Carbon (primary production)

2 kg CO₂/kg
1.9 kg CO₂/kg
2 kg CO₂/kg
2.1 kg CO₂/kg

Embodied Water

40 L/kg4.8 gal/lb
40 L/kg4.8 gal/lb
45 L/kg5.4 gal/lb
50 L/kg6 gal/lb

Typical Recycled Content

25%
30%
30%
25%

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

83 kN·m/kg
60 kN·m/kg
75 kN·m/kg
79 kN·m/kg

Specific Stiffness (E / density)

26.8 MN·m/kg
26.1 MN·m/kg
26.1 MN·m/kg
26.1 MN·m/kg

Modulus of Resilience

572 kJ/m³
165 kJ/m³
250 kJ/m³
420 kJ/m³

Thermal Diffusivity

12.2 mm²/s
13.6 mm²/s
12.8 mm²/s
13.4 mm²/s

Thermal Shock Resistance Index

12
10
12
13

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale103010351040E355

Manufacturing and finishing

CapabilityE355103010351040
Default conditionCDHRHRHR
Relative cost$$ Standard$ Budget$ Budget$ Budget
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining and Sheet metal. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in E355 and 1030 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.