FabDigit

Cronidur 30 vs 52100 and 2 more: properties

Cronidur 3052100SUJ2100Cr6

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

200 GPa29 Msi
205 GPa29.7 Msi
210 GPa30.5 Msi
210 GPa30.5 Msi

Shear Modulus

78 GPa11.3 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi

Bulk Modulus

165 GPa23.9 Msi
166 GPa24.1 Msi
160 GPa23.2 Msi
160 GPa23.2 Msi

Poisson's Ratio

0.29
0.3
0.29
0.29

Tensile Strength (Ultimate)

2,100 MPa305 ksi
690 MPa100 ksi
660 MPa95.7 ksi
660 MPa95.7 ksi

Yield Strength (0.2% offset)

1,850 MPa268 ksi
415 MPa60.2 ksi
420 MPa60.9 ksi
420 MPa60.9 ksi

Elongation at Break

4%
25%
25%
22%

Reduction in Area

10%
45%
45%
48%

Compressive Strength

2,600 MPa377 ksi
430 MPa62.4 ksi
450 MPa65.3 ksi

Shear Strength

1,300 MPa189 ksi
420 MPa60.9 ksi
400 MPa58 ksi
400 MPa58 ksi

Fatigue Strength (Endurance Limit)

950 MPa138 ksi
320 MPa46.4 ksi
320 MPa46.4 ksi
300 MPa43.5 ksi

Fracture Toughness (K_IC)

20 MPa·√m18.2 ksi·√in

Charpy V-Notch Impact (RT)

10 J7.4 ft·lbf
15 J11.1 ft·lbf
30 J22.1 ft·lbf
25 J18.4 ft·lbf

Hardness, Rockwell C

59 HRC

Hardness, Vickers

680 HV
205 HV
200 HV
210 HV

Hardness, Brinell

195 HB
192 HB
200 HB

Hardness, Rockwell B

93 HRB
92 HRB
94 HRB

Physical

Density and transition temperatures.

Density

7.7 g/cm³0.28 lb/in³
7.81 g/cm³0.28 lb/in³
7.81 g/cm³0.28 lb/in³
7.81 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,400°C2,552 °F
1,424°C2,595 °F
1,425°C2,597 °F
1,424°C2,595 °F

Liquidus Temperature

1,450°C2,642 °F
1,455°C2,651 °F
1,460°C2,660 °F
1,455°C2,651 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

16 W/m·K9.2 BTU/hr·ft·°F
46 W/m·K26.6 BTU/hr·ft·°F
46 W/m·K26.6 BTU/hr·ft·°F
45 W/m·K26 BTU/hr·ft·°F

Specific Heat Capacity

460 J/kg·K0.11 BTU/lb·°F
475 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

10.5 µm/m·K5.8 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F

Latent Heat of Fusion

270 J/g116 BTU/lb
247 J/g106 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Max Service Temperature (continuous)

250°C482 °F
400°C752 °F
200°C392 °F
200°C392 °F

Min Service Temperature

-253°C-423 °F
-40°C-40 °F
-40°C-40 °F
-40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

2.3 % IACS
7 % IACS
7 % IACS
8 % IACS

Electrical Resistivity

7.5×10⁻⁷ Ω·m29.5 µΩ·in
2.5×10⁻⁷ Ω·m9.84 µΩ·in
2.5×10⁻⁷ Ω·m9.84 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.2 V
-0.62 V
-0.61 V
-0.6 V

Corrosion Resistance

58 / 100
12 / 100
12 / 100
12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

12 / 100
40 / 100
45 / 100
45 / 100

Machinability Rating (AISI 1212 = 100 %)

8%
40%
40%
40%

Weldability

15 / 100
12 / 100
12 / 100
12 / 100

Formability (cold)

5 / 100
35 / 100
35 / 100
35 / 100

Brazeability / Solderability

25 / 100
35 / 100
35 / 100
45 / 100

Polishability

90 / 100
85 / 100
85 / 100
88 / 100

Castability

25 / 100
30 / 100
30 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

85 MJ/kg36,543 BTU/lb
30 MJ/kg12,898 BTU/lb
30 MJ/kg12,898 BTU/lb
32 MJ/kg13,758 BTU/lb

Embodied Carbon (primary production)

5.5 kg CO₂/kg
2.2 kg CO₂/kg
2.3 kg CO₂/kg
2.3 kg CO₂/kg

Embodied Water

200 L/kg24 gal/lb
55 L/kg6.6 gal/lb
55 L/kg6.6 gal/lb
65 L/kg7.8 gal/lb

Typical Recycled Content

25%
30%
30%
30%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

273 kN·m/kg
88 kN·m/kg
85 kN·m/kg
85 kN·m/kg

Specific Stiffness (E / density)

26 MN·m/kg
26.2 MN·m/kg
26.9 MN·m/kg
26.9 MN·m/kg

Modulus of Resilience

8,556 kJ/m³
420 kJ/m³
420 kJ/m³
420 kJ/m³

Thermal Diffusivity

4.5 mm²/s
12.4 mm²/s
12.8 mm²/s
12.3 mm²/s

Thermal Shock Resistance Index

16
13
12
12

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale52100SUJ2100Cr6Cronidur 30

Manufacturing and finishing

CapabilityCronidur 3052100SUJ2100Cr6
CNC machiningYesYesYes
Sheet metalYesYesYes
Default conditionAnnealedAnnealedAnnealed
Relative cost$$$$ High$$$ Premium$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µm
AlCrNYesYesYes
AlTiNYesYesYes
Black OxideYesYesYes
CVD Al2O3YesYesYes
CVD TiCNYesYesYes
CVD TiNYesYesYes
CerakoteYesYesYes
Chrome PlatingYesYesYes
CrNYesYesYes
DLCYesYesYes
E-CoatingYesYesYes
HVOF CoatingYesYesYes
Hot-Dip GalvanizingYesYesYes
MoS2YesYesYes
Multilayer CVDYesYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Cronidur 30 and 52100 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.