Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

207 GPa30 Msi
206 GPa29.9 Msi
210 GPa30.5 Msi
210 GPa30.5 Msi

Shear Modulus

80 GPa11.6 Msi
79.5 GPa11.5 Msi
80 GPa11.6 Msi
80 GPa11.6 Msi

Tensile Strength (Ultimate)

1,250 MPa181 ksi
800 MPa116 ksi
850 MPa123 ksi
620 MPa89.9 ksi

Yield Strength (0.2% offset)

1,050 MPa152 ksi
480 MPa69.6 ksi
550 MPa79.8 ksi
420 MPa60.9 ksi

Elongation at Break

12%
16%
14%
14%

Reduction in Area

45%
40%
40%
45%

Compressive Strength

1,080 MPa157 ksi
480 MPa69.6 ksi
560 MPa81.2 ksi

Shear Strength

750 MPa109 ksi
500 MPa72.5 ksi
510 MPa74 ksi
400 MPa58 ksi

Fatigue Strength (Endurance Limit)

550 MPa79.8 ksi
360 MPa52.2 ksi
400 MPa58 ksi
280 MPa40.6 ksi

Fracture Toughness (K_IC)

90 MPa·√m81.9 ksi·√in
85 MPa·√m77.4 ksi·√in
75 MPa·√m68.3 ksi·√in
55 MPa·√m50.1 ksi·√in

Charpy V-Notch Impact (RT)

40 J29.5 ft·lbf
30 J22.1 ft·lbf
30 J22.1 ft·lbf
40 J29.5 ft·lbf

Hardness, Brinell

375 HB
225 HB
245 HB
185 HB

Hardness, Rockwell C

40 HRC
20 HRC
23 HRC

Hardness, Vickers

395 HV
236 HV
258 HV
195 HV

Hardness, Rockwell B

98 HRB
89 HRB

Same in both: Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Liquidus Temperature

1,490°C2,714 °F
1,490°C2,714 °F
1,495°C2,723 °F
1,495°C2,723 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

32 W/m·K18.5 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F
42.6 W/m·K24.6 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F

Specific Heat Capacity

460 J/kg·K0.11 BTU/lb·°F
465 J/kg·K0.11 BTU/lb·°F
473 J/kg·K0.11 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.5 µm/m·K6.4 µin/in·°F
12.5 µm/m·K6.9 µin/in·°F
12.3 µm/m·K6.8 µin/in·°F
12.5 µm/m·K6.9 µin/in·°F

Latent Heat of Fusion

270 J/g116 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb

Min Service Temperature

-80°C-112 °F
-40°C-40 °F
-40°C-40 °F
-40°C-40 °F

Same in both: Max Service Temperature (continuous) 400°C752 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

3×10⁻⁷ Ω·m11.8 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in
2.2×10⁻⁷ Ω·m8.66 µΩ·in

Electrical Conductivity

7.8 % IACS
7.8 % IACS
8 % IACS

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

13 / 100
10 / 100
12 / 100
11 / 100

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.6 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

32 / 100
50 / 100
50 / 100
55 / 100

Machinability Rating (AISI 1212 = 100 %)

35%
55%
55%
60%

Weldability

22 / 100
25 / 100
35 / 100
55 / 100

Formability (cold)

18 / 100
45 / 100
35 / 100
60 / 100

Brazeability / Solderability

40 / 100
40 / 100
50 / 100
45 / 100

Polishability

70 / 100
60 / 100
70 / 100
55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

34 MJ/kg14,617 BTU/lb
26 MJ/kg11,178 BTU/lb
30 MJ/kg12,898 BTU/lb
25 MJ/kg10,748 BTU/lb

Embodied Carbon (primary production)

2.5 kg CO₂/kg
2 kg CO₂/kg
2.2 kg CO₂/kg
2 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
45 L/kg5.4 gal/lb
60 L/kg7.2 gal/lb
40 L/kg4.8 gal/lb

Typical Recycled Content

30%
30%
30%
25%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

159 kN·m/kg
102 kN·m/kg
108 kN·m/kg
79 kN·m/kg

Specific Stiffness (E / density)

26.4 MN·m/kg
26.2 MN·m/kg
26.8 MN·m/kg
26.8 MN·m/kg

Modulus of Resilience

2,663 kJ/m³
559 kJ/m³
720 kJ/m³
420 kJ/m³

Thermal Diffusivity

8.9 mm²/s
12.1 mm²/s
11.5 mm²/s
11.9 mm²/s

Thermal Shock Resistance Index

17
14
14
10

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale55Cr342CrMo434MnB533NiCrMoV14-5

Manufacturing and finishing

Capability33NiCrMoV14-555Cr342CrMo434MnB5
CNC machiningYesYes
Sheet metalYesYesYes
Default conditionAnnealedHRCR
Relative cost$$$ Premium$$ Standard$$ Standard$$ Standard
Min. machined wall0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µm
AlCrNYesYes
AlTiNYesYes
Black OxideYesYesYes
CVD Al2O3YesYes
CVD TiCNYesYes
CVD TiNYesYes
CerakoteYesYesYes
Chrome PlatingYesYesYes
CrNYesYes
DLCYesYes
E-CoatingYesYesYes
HVOF CoatingYesYes
Hot-Dip GalvanizingYesYesYes
MoS2YesYes
Multilayer CVDYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes

They share 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 33NiCrMoV14-5 and 55Cr3 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.