FabDigit

1137 vs 1117 and 2 more: properties

1137111711411215

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

205 GPa29.7 Msi
200 GPa29 Msi
200 GPa29 Msi
200 GPa29 Msi

Tensile Strength (Ultimate)

620 MPa89.9 ksi
425 MPa61.6 ksi
675 MPa97.9 ksi
415 MPa60.2 ksi

Yield Strength (0.2% offset)

380 MPa55.1 ksi
235 MPa34.1 ksi
360 MPa52.2 ksi
250 MPa36.3 ksi

Elongation at Break

15%
33%
22%
25%

Reduction in Area

35%
58%
38%
45%

Shear Strength

400 MPa58 ksi
320 MPa46.4 ksi
405 MPa58.7 ksi
290 MPa42.1 ksi

Fatigue Strength (Endurance Limit)

280 MPa40.6 ksi
200 MPa29 ksi
300 MPa43.5 ksi
190 MPa27.6 ksi

Charpy V-Notch Impact (RT)

60 J44.3 ft·lbf
50 J36.9 ft·lbf
30 J22.1 ft·lbf

Hardness, Brinell

179 HB
121 HB
192 HB
121 HB

Hardness, Rockwell B

89 HRB
68 HRB
92 HRB
70 HRB

Same in both: Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Density

7.85 g/cm³0.28 lb/in³
7.87 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³
7.87 g/cm³0.28 lb/in³

Melting Point (Solidus)

1,425°C2,597 °F
1,420°C2,588 °F
1,425°C2,597 °F
1,420°C2,588 °F

Liquidus Temperature

1,500°C2,732 °F
1,500°C2,732 °F
1,490°C2,714 °F
1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

48 W/m·K27.7 BTU/hr·ft·°F
51 W/m·K29.5 BTU/hr·ft·°F
49 W/m·K28.3 BTU/hr·ft·°F
51.9 W/m·K30 BTU/hr·ft·°F

Specific Heat Capacity

486 J/kg·K0.12 BTU/lb·°F
470 J/kg·K0.11 BTU/lb·°F
486 J/kg·K0.12 BTU/lb·°F
486 J/kg·K0.12 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

11.7 µm/m·K6.5 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
11.7 µm/m·K6.5 µin/in·°F
11.9 µm/m·K6.6 µin/in·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
250 J/g107 BTU/lb
250 J/g107 BTU/lb
247 J/g106 BTU/lb

Max Service Temperature (continuous)

400°C752 °F
400°C752 °F
425°C797 °F
400°C752 °F

Same in both: Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

10 % IACS
10.8 % IACS
9.5 % IACS
10.8 % IACS

Electrical Resistivity

1.7×10⁻⁷ Ω·m6.69 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in
1.8×10⁻⁷ Ω·m7.09 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

9 / 100
10 / 100
10 / 100
8 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

70 / 100
70 / 100
68 / 100
85 / 100

Machinability Rating (AISI 1212 = 100 %)

70%
91%
70%
120%

Weldability

25 / 100
50 / 100
25 / 100
20 / 100

Formability (cold)

35 / 100
60 / 100
35 / 100
35 / 100

Brazeability / Solderability

55 / 100
65 / 100
55 / 100
55 / 100

Polishability

40 / 100
45 / 100
55 / 100
40 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb
25 MJ/kg10,748 BTU/lb
26 MJ/kg11,178 BTU/lb

Embodied Carbon (primary production)

1.9 kg CO₂/kg
1.9 kg CO₂/kg
1.9 kg CO₂/kg
2 kg CO₂/kg

Typical Recycled Content

40%
30%
30%
35%

Same in both: Embodied Water 45 L/kg5.4 gal/lb

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

79 kN·m/kg
54 kN·m/kg
86 kN·m/kg
53 kN·m/kg

Specific Stiffness (E / density)

26.1 MN·m/kg
25.4 MN·m/kg
25.5 MN·m/kg
25.4 MN·m/kg

Modulus of Resilience

352 kJ/m³
138 kJ/m³
324 kJ/m³
156 kJ/m³

Thermal Diffusivity

12.6 mm²/s
13.8 mm²/s
12.8 mm²/s
13.6 mm²/s

Thermal Shock Resistance Index

12
9
14
9

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale1117114112151137

Manufacturing and finishing

Capability1137111711411215
Default conditionHRHRHRHR
Relative cost$ Budget$ Budget$$ Standard$ Budget
Min. machined wall0.8 mm0.8 mm0.8 mm0.8 mm
Best machined surfaceRa 1.6 µmRa 1.6 µmRa 1.6 µmRa 1.6 µm

Both are offered for CNC machining. Both take the same 38 finishes: AlCrN, AlTiN, Black Oxide, CVD Al2O3, CVD TiCN, CVD TiN, Cerakote, Chrome Plating, Copper Plating, CrN, DLC, E-Coating and 26 more.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 1137 and 1117 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.