ZL207 vs ZL102 and 2 more: properties

ZL207ZL102ZL205AZL301

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

70 GPa10.2 Msi
71 GPa10.3 Msi
70 GPa10.2 Msi
68 GPa9.9 Msi

Shear Modulus

26.5 GPa3.8 Msi
26.5 GPa3.8 Msi
26.5 GPa3.8 Msi
25.5 GPa3.7 Msi

Bulk Modulus

71 GPa10.3 Msi
70 GPa10.2 Msi
70 GPa10.2 Msi
66 GPa9.6 Msi

Tensile Strength (Ultimate)

185 MPa26.8 ksi
170 MPa24.7 ksi
460 MPa66.7 ksi
160 MPa23.2 ksi

Yield Strength (0.2% offset)

150 MPa21.8 ksi
80 MPa11.6 ksi
320 MPa46.4 ksi
110 MPa16 ksi

Elongation at Break

1.5%
5%
9%
3%

Shear Strength

130 MPa18.9 ksi
120 MPa17.4 ksi
275 MPa39.9 ksi
110 MPa16 ksi

Fatigue Strength (Endurance Limit)

70 MPa10.2 ksi
70 MPa10.2 ksi
105 MPa15.2 ksi
45 MPa6.5 ksi

Hardness, Brinell

80 HB
55 HB
105 HB
55 HB

Fracture Toughness (K_IC)

17 MPa·√m15.5 ksi·√in
27 MPa·√m24.6 ksi·√in

Charpy V-Notch Impact (RT)

4 J3 ft·lbf
12 J8.9 ft·lbf
4 J3 ft·lbf

Hardness, Vickers

60 HV
112 HV

Compressive Strength

330 MPa47.9 ksi
165 MPa23.9 ksi

Same in both: Poisson's Ratio 0.33

Physical

Density and transition temperatures.

Density

2.85 g/cm³0.1 lb/in³
2.65 g/cm³0.1 lb/in³
2.82 g/cm³0.1 lb/in³
2.57 g/cm³0.09 lb/in³

Melting Point (Solidus)

545°C1,013 °F
574°C1,065 °F
545°C1,013 °F
450°C842 °F

Liquidus Temperature

640°C1,184 °F
582°C1,080 °F
650°C1,202 °F
600°C1,112 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

130 W/m·K75.1 BTU/hr·ft·°F
145 W/m·K83.8 BTU/hr·ft·°F
150 W/m·K86.7 BTU/hr·ft·°F
100 W/m·K57.8 BTU/hr·ft·°F

Specific Heat Capacity

880 J/kg·K0.21 BTU/lb·°F
963 J/kg·K0.23 BTU/lb·°F
880 J/kg·K0.21 BTU/lb·°F
963 J/kg·K0.23 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

21 µm/m·K11.7 µin/in·°F
20.5 µm/m·K11.4 µin/in·°F
22.5 µm/m·K12.5 µin/in·°F
25.2 µm/m·K14 µin/in·°F

Latent Heat of Fusion

390 J/g168 BTU/lb
389 J/g167 BTU/lb
390 J/g168 BTU/lb
380 J/g163 BTU/lb

Max Service Temperature (continuous)

350°C662 °F
150°C302 °F
175°C347 °F
100°C212 °F

Same in both: Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

32 % IACS
31 % IACS
33 % IACS
24 % IACS

Electrical Resistivity

5.4×10⁻⁸ Ω·m2.13 µΩ·in
5.6×10⁻⁸ Ω·m2.2 µΩ·in
5.2×10⁻⁸ Ω·m2.05 µΩ·in
8.2×10⁻⁸ Ω·m3.23 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.72 V
-0.83 V
-0.73 V
-0.87 V

Corrosion Resistance

33 / 100
60 / 100
30 / 100
62 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
45 / 100
75 / 100
78 / 100

Machinability Rating (AISI 1212 = 100 %)

100%
40%
150%
300%

Weldability

25 / 100
75 / 100
45 / 100
45 / 100

Formability (cold)

5 / 100
10 / 100
10 / 100
10 / 100

Castability

50 / 100
98 / 100
40 / 100
30 / 100

Brazeability / Solderability

20 / 100
45 / 100
25 / 100
10 / 100

Polishability

40 / 100
40 / 100
55 / 100
75 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

200 MJ/kg85,985 BTU/lb
200 MJ/kg85,985 BTU/lb
200 MJ/kg85,985 BTU/lb
195 MJ/kg83,835 BTU/lb

Embodied Carbon (primary production)

13 kg CO₂/kg
11.5 kg CO₂/kg
12.5 kg CO₂/kg
13.5 kg CO₂/kg

Embodied Water

1,100 L/kg132 gal/lb
1,150 L/kg138 gal/lb
1,150 L/kg138 gal/lb
1,150 L/kg138 gal/lb

Typical Recycled Content

15%
70%
10%
15%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

65 kN·m/kg
64 kN·m/kg
163 kN·m/kg
62 kN·m/kg

Specific Stiffness (E / density)

24.6 MN·m/kg
26.8 MN·m/kg
24.8 MN·m/kg
26.5 MN·m/kg

Modulus of Resilience

161 kJ/m³
45 kJ/m³
731 kJ/m³
89 kJ/m³

Thermal Diffusivity

51.8 mm²/s
56.8 mm²/s
60.4 mm²/s
40.4 mm²/s

Thermal Shock Resistance Index

16
17
44
9

Strength versus weight

Yield strength against density for every aluminum grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

20501002005002.22.42.62.83Density (g/cm³)Yield strength (MPa) — log scaleZL102ZL205AZL301ZL207

Manufacturing and finishing

CapabilityZL207ZL102ZL205AZL301
CNC machiningYesYesYes
Default conditionFT5F
Relative cost$$$ Premium$ Budget$$$$ High$$ Standard
Min. machined wall0.5 mm0.5 mm0.5 mm
Best machined surfaceRa 0.8 µmRa 0.8 µmRa 0.8 µm
Anodizing Type IIYesYesYes
CerakoteYesYesYes
Chem Film (Alodine)YesYesYes
DLCYesYesYes
E-CoatingYesYesYes
ElectropolishingYesYesYes
Hard Anodize Type III w/ PTFEYesYesYes
Hard Anodizing Type IIIYesYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes
Powder CoatingYesYesYes

They share 4 finishes: Electroless Nickel (EN), Epoxy Coating, Gold Plating, Silver Plating.

Ready to make it?

Upload a CAD file and FabDigit prices the part in ZL207 and ZL102 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.