FabDigitFabDigit

Steel Y20-N vs Y20-QT

Steel · Y20 temper comparison

Y20-N and Y20-QT are two conditions of the same steel grade, Y20: N (normalized) versus QT (quenched and tempered). The chemistry is identical, so every difference below comes from the condition. Y20-QT is the stronger of the two: yield strength 440 MPa (63.8 ksi) against 300 MPa (43.5 ksi) for Y20-N, about 47% more; tensile strength follows at 620 MPa (89.9 ksi) vs 490 MPa (71.1 ksi). In exchange, Y20-N is the more ductile: elongation 25% versus 20% for Y20-QT, and Y20-QT is harder (190 HB vs 148 HB). Y20-QT runs hotter in service (450°C vs 400°C continuous).

Y20-NChoose it when the part is bent, formed or impact-loaded.

Y20-QTChoose it when strength drives the design, or when the part sees heat.

Y20-N vs Y20-QT: properties

Y20-NY20-QT

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

490 MPa71.1 ksi
620 MPa89.9 ksi

Yield Strength (0.2% offset)

300 MPa43.5 ksi
440 MPa63.8 ksi

Elongation at Break

25%
20%

Reduction in Area

45%
50%

Compressive Strength

300 MPa43.5 ksi
440 MPa63.8 ksi

Shear Strength

330 MPa47.9 ksi
400 MPa58 ksi

Fatigue Strength (Endurance Limit)

235 MPa34.1 ksi
280 MPa40.6 ksi

Charpy V-Notch Impact (RT)

50 J36.9 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

148 HB
190 HB

Hardness, Rockwell B

79 HRB
92 HRB

Hardness, Vickers

155 HV
200 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,505°C2,741 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

51 W/m·K29.5 BTU/hr·ft·°F
49 W/m·K28.3 BTU/hr·ft·°F

Max Service Temperature (continuous)

400°C752 °F
450°C842 °F

Same in both: Specific Heat Capacity 480 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.9 µm/m·K6.6 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

10.5 % IACS
9.8 % IACS

Electrical Resistivity

1.65×10⁻⁷ Ω·m6.5 µΩ·in
1.75×10⁻⁷ Ω·m6.89 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 9 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

72 / 100
70 / 100

Machinability Rating (AISI 1212 = 100 %)

72%
70%

Weldability

35 / 100
30 / 100

Formability (cold)

58 / 100
35 / 100

Same in both: Castability 40 / 100 · Brazeability / Solderability 60 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 1.9 kg CO₂/kg · Embodied Water 50 L/kg6 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleY20

Y20-N vs Y20-QT — frequently asked

Is Y20-QT stronger than Y20-N?

Yes. Y20-QT has a typical yield strength of 440 MPa (63.8 ksi) against 300 MPa (43.5 ksi) for Y20-N — about 47% more. Tensile strength is 620 MPa (89.9 ksi) vs 490 MPa (71.1 ksi).

Which condition does FabDigit quote by default, N or QT?

CD is the default Y20 condition in the FabDigit quote flow (neither N nor QT). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, Y20-N or Y20-QT?

Y20-N. Its weldability rates fair (35/100) against poor (30/100) for Y20-QT.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Y20-N and Y20-QT side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.