FabDigitFabDigit

Steel SUM32-HR vs SUM32-N

Steel · SUM32 temper comparison

SUM32-HR and SUM32-N are two conditions of the same steel grade, SUM32: HR (hot rolled) versus N (normalized). The chemistry is identical, so every difference below comes from the condition. SUM32-N is the stronger of the two: yield strength 303 MPa (43.9 ksi) against 235 MPa (34.1 ksi) for SUM32-HR, about 29% more; tensile strength follows at 467 MPa (67.7 ksi) vs 425 MPa (61.6 ksi).

SUM32-NChoose it when strength drives the design.

SUM32-HR vs SUM32-N: properties

SUM32-HRSUM32-N

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

425 MPa61.6 ksi
467 MPa67.7 ksi

Yield Strength (0.2% offset)

235 MPa34.1 ksi
303 MPa43.9 ksi

Elongation at Break

33%
33.5%

Reduction in Area

63%
64%

Shear Strength

290 MPa42.1 ksi
280 MPa40.6 ksi

Fatigue Strength (Endurance Limit)

205 MPa29.7 ksi
225 MPa32.6 ksi

Charpy V-Notch Impact (RT)

70 J51.6 ft·lbf
84 J62 ft·lbf

Hardness, Rockwell B

68 HRB
69 HRB

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Hardness, Brinell 121 HB

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

51.9 W/m·K30 BTU/hr·ft·°F
51.5 W/m·K29.8 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 486 J/kg·K0.12 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 350°C662 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1.6×10⁻⁷ Ω·m6.3 µΩ·in
1.62×10⁻⁷ Ω·m6.38 µΩ·in

Same in both: Electrical Conductivity 10.5 % IACS

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

80 / 100
82 / 100

Machinability Rating (AISI 1212 = 100 %)

85%
88%

Weldability

40 / 100
45 / 100

Same in both: Formability (cold) 55 / 100 · Brazeability / Solderability 65 / 100 · Polishability 40 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 1.9 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSUM32

SUM32-HR vs SUM32-N — frequently asked

Is SUM32-N stronger than SUM32-HR?

Yes. SUM32-N has a typical yield strength of 303 MPa (43.9 ksi) against 235 MPa (34.1 ksi) for SUM32-HR — about 29% more. Tensile strength is 467 MPa (67.7 ksi) vs 425 MPa (61.6 ksi).

Which condition does FabDigit quote by default, HR or N?

CD is the default SUM32 condition in the FabDigit quote flow (neither HR nor N). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, SUM32-HR or SUM32-N?

SUM32-N. Its weldability rates fair (45/100) against fair (40/100) for SUM32-HR.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SUM32-HR and SUM32-N side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.