FabDigitFabDigit

Steel SUM32-A vs SUM32-CD

Steel · SUM32 temper comparison

SUM32-A and SUM32-CD are two conditions of the same steel grade, SUM32: A (solution annealed) versus CD (cold drawn). The chemistry is identical, so every difference below comes from the condition. SUM32-CD is the stronger of the two: yield strength 415 MPa (60.2 ksi) against 285 MPa (41.3 ksi) for SUM32-A, about 46% more; tensile strength follows at 485 MPa (70.3 ksi) vs 430 MPa (62.4 ksi). In exchange, SUM32-A is the more ductile: elongation 33% versus 15% for SUM32-CD, and SUM32-CD is harder (143 HB vs 121 HB).

SUM32-AChoose it when the part is bent, formed or impact-loaded.

SUM32-CDChoose it when strength drives the design.

SUM32-A vs SUM32-CD: properties

SUM32-ASUM32-CD

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

430 MPa62.4 ksi
485 MPa70.3 ksi

Yield Strength (0.2% offset)

285 MPa41.3 ksi
415 MPa60.2 ksi

Elongation at Break

33%
15%

Reduction in Area

63%
40%

Shear Strength

260 MPa37.7 ksi
290 MPa42.1 ksi

Fatigue Strength (Endurance Limit)

210 MPa30.5 ksi
240 MPa34.8 ksi

Charpy V-Notch Impact (RT)

75 J55.3 ft·lbf
40 J29.5 ft·lbf

Hardness, Brinell

121 HB
143 HB

Hardness, Rockwell B

68 HRB
78 HRB

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

52.5 W/m·K30.3 BTU/hr·ft·°F
51.9 W/m·K30 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 486 J/kg·K0.12 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 350°C662 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

10.8 % IACS
10.5 % IACS

Same in both: Electrical Resistivity 1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

80 / 100
85 / 100

Machinability Rating (AISI 1212 = 100 %)

85%
91%

Weldability

45 / 100
40 / 100

Formability (cold)

60 / 100
40 / 100

Same in both: Brazeability / Solderability 65 / 100 · Polishability 40 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 1.9 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSUM32

SUM32-A vs SUM32-CD — frequently asked

Is SUM32-CD stronger than SUM32-A?

Yes. SUM32-CD has a typical yield strength of 415 MPa (60.2 ksi) against 285 MPa (41.3 ksi) for SUM32-A — about 46% more. Tensile strength is 485 MPa (70.3 ksi) vs 430 MPa (62.4 ksi).

Which condition does FabDigit quote by default, A or CD?

CD is the default SUM32 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, SUM32-A or SUM32-CD?

SUM32-CD. Its machinability rates excellent (85/100) against very good (80/100) for SUM32-A; for welding the order is SUM32-A first (fair, 45/100) then SUM32-CD (fair, 40/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in SUM32-A and SUM32-CD side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.