FabDigitFabDigit

Steel SUJ3-CD vs SUJ3-N

Steel · SUJ3 temper comparison

SUJ3-CD and SUJ3-N are two conditions of the same steel grade, SUJ3: CD (cold drawn) versus N (normalized). The chemistry is identical, so every difference below comes from the condition. SUJ3-N is the stronger of the two: tensile strength 1,050 MPa (152 ksi) against 820 MPa (119 ksi) for SUJ3-CD, about 28% more. In exchange, SUJ3-CD is the more ductile: elongation 10% versus 9% for SUJ3-N, and SUJ3-N is harder (320 HB vs 250 HB). On the shop floor, SUJ3-CD machines more easily (fair vs poor).

SUJ3-CDChoose it when the part is bent, formed or impact-loaded, or when the part is machined in volume.

SUJ3-NChoose it when strength drives the design.

SUJ3-CD vs SUJ3-N: properties

SUJ3-CDSUJ3-N

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

820 MPa119 ksi
1,050 MPa152 ksi

Yield Strength (0.2% offset)

640 MPa92.8 ksi
650 MPa94.3 ksi

Elongation at Break

10%
9%

Reduction in Area

35%
22%

Compressive Strength

860 MPa125 ksi
1,100 MPa160 ksi

Shear Strength

500 MPa72.5 ksi
630 MPa91.4 ksi

Fatigue Strength (Endurance Limit)

370 MPa53.7 ksi
470 MPa68.2 ksi

Charpy V-Notch Impact (RT)

12 J8.9 ft·lbf
7 J5.2 ft·lbf

Hardness, Brinell

250 HB
320 HB

Hardness, Rockwell B

101 HRB
92 HRB

Hardness, Vickers

262 HV
335 HV

Same in both: Elastic (Young's) Modulus 208 GPa30.2 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.81 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,400°C2,552 °F · Liquidus Temperature 1,450°C2,642 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

44 W/m·K25.4 BTU/hr·ft·°F
41 W/m·K23.7 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

42 / 100
22 / 100

Machinability Rating (AISI 1212 = 100 %)

38%
20%

Weldability

6 / 100
5 / 100

Formability (cold)

20 / 100
10 / 100

Same in both: Brazeability / Solderability 40 / 100 · Polishability 85 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 31 MJ/kg13,328 BTU/lb · Embodied Carbon (primary production) 2.2 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSUJ3

SUJ3-CD vs SUJ3-N — frequently asked

Is SUJ3-N stronger than SUJ3-CD?

Yes. SUJ3-N has a typical tensile strength of 1,050 MPa (152 ksi) against 820 MPa (119 ksi) for SUJ3-CD — about 28% more.

Which condition does FabDigit quote by default, CD or N?

A is the default SUJ3 condition in the FabDigit quote flow (neither CD nor N). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, SUJ3-CD or SUJ3-N?

SUJ3-CD. Its machinability rates fair (42/100) against poor (22/100) for SUJ3-N.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SUJ3-CD and SUJ3-N side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.