FabDigitFabDigit

Steel SS490-CD vs SS490-SR

Steel · SS490 temper comparison

SS490-CD and SS490-SR are two conditions of the same steel grade, SS490: CD (cold drawn) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. SS490-CD is the stronger of the two: yield strength 490 MPa (71.1 ksi) against 305 MPa (44.2 ksi) for SS490-SR, about 61% more; tensile strength follows at 600 MPa (87 ksi) vs 515 MPa (74.7 ksi). In exchange, SS490-SR is the more ductile: elongation 24% versus 12% for SS490-CD, and SS490-CD is harder (180 HB vs 148 HB). SS490-SR runs hotter in service (350°C vs 300°C continuous).

SS490-CDChoose it when strength drives the design.

SS490-SRChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

SS490-CD vs SS490-SR: properties

SS490-CDSS490-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

600 MPa87 ksi
515 MPa74.7 ksi

Yield Strength (0.2% offset)

490 MPa71.1 ksi
305 MPa44.2 ksi

Elongation at Break

12%
24%

Reduction in Area

40%
47%

Compressive Strength

490 MPa71.1 ksi
305 MPa44.2 ksi

Shear Strength

400 MPa58 ksi
345 MPa50 ksi

Fatigue Strength (Endurance Limit)

265 MPa38.4 ksi
235 MPa34.1 ksi

Fracture Toughness (K_IC)

70 MPa·√m63.7 ksi·√in
88 MPa·√m80.1 ksi·√in

Charpy V-Notch Impact (RT)

25 J18.4 ft·lbf
50 J36.9 ft·lbf

Hardness, Brinell

180 HB
148 HB

Hardness, Rockwell B

89 HRB
79 HRB

Hardness, Vickers

190 HV
156 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

300°C572 °F
350°C662 °F

Same in both: Thermal Conductivity 50 W/m·K28.9 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.65 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

66 / 100
58 / 100

Machinability Rating (AISI 1212 = 100 %)

70%
62%

Weldability

70 / 100
78 / 100

Formability (cold)

40 / 100
62 / 100

Same in both: Brazeability / Solderability 60 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSS490

SS490-CD vs SS490-SR — frequently asked

Is SS490-CD stronger than SS490-SR?

Yes. SS490-CD has a typical yield strength of 490 MPa (71.1 ksi) against 305 MPa (44.2 ksi) for SS490-SR — about 61% more. Tensile strength is 600 MPa (87 ksi) vs 515 MPa (74.7 ksi).

Which condition does FabDigit quote by default, CD or SR?

HR is the default SS490 condition in the FabDigit quote flow (neither CD nor SR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, SS490-CD or SS490-SR?

SS490-CD, by a small margin. Both rate good for machinability — 66/100 against 58/100 for SS490-SR; for welding the order is SS490-SR first (very good, 78/100) then SS490-CD (very good, 70/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in SS490-CD and SS490-SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.