FabDigitFabDigit

Steel SNCM447-CD vs SNCM447-N

Steel · SNCM447 temper comparison

SNCM447-CD and SNCM447-N are two conditions of the same steel grade, SNCM447: CD (cold drawn) versus N (normalized). The chemistry is identical, so every difference below comes from the condition. SNCM447-CD is the stronger of the two: yield strength 730 MPa (106 ksi) against 620 MPa (89.9 ksi) for SNCM447-N, about 18% more. In exchange, SNCM447-N is the more ductile: elongation 14% versus 12% for SNCM447-CD, and SNCM447-N is harder (285 HB vs 255 HB).

SNCM447-CDChoose it when strength drives the design.

SNCM447-NChoose it when the part is bent, formed or impact-loaded.

SNCM447-CD vs SNCM447-N: properties

SNCM447-CDSNCM447-N

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

880 MPa128 ksi
950 MPa138 ksi

Yield Strength (0.2% offset)

730 MPa106 ksi
620 MPa89.9 ksi

Elongation at Break

12%
14%

Reduction in Area

30%
38%

Compressive Strength

740 MPa107 ksi
630 MPa91.4 ksi

Shear Strength

530 MPa76.9 ksi
570 MPa82.7 ksi

Fatigue Strength (Endurance Limit)

390 MPa56.6 ksi
430 MPa62.4 ksi

Fracture Toughness (K_IC)

50 MPa·√m45.5 ksi·√in
55 MPa·√m50.1 ksi·√in

Charpy V-Notch Impact (RT)

14 J10.3 ft·lbf
20 J14.8 ft·lbf

Hardness, Brinell

255 HB
285 HB

Hardness, Rockwell C

25 HRC
29 HRC

Hardness, Vickers

270 HV
300 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,490°C2,714 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 44 W/m·K25.4 BTU/hr·ft·°F · Specific Heat Capacity 475 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.3 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -50°C-58 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7 % IACS · Electrical Resistivity 2.45×10⁻⁷ Ω·m9.65 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

52 / 100
45 / 100

Machinability Rating (AISI 1212 = 100 %)

58%
45%

Weldability

28 / 100
30 / 100

Formability (cold)

25 / 100
28 / 100

Same in both: Brazeability / Solderability 45 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.3 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSNCM447

SNCM447-CD vs SNCM447-N — frequently asked

Is SNCM447-CD stronger than SNCM447-N?

Yes. SNCM447-CD has a typical yield strength of 730 MPa (106 ksi) against 620 MPa (89.9 ksi) for SNCM447-N — about 18% more. Tensile strength is 880 MPa (128 ksi) vs 950 MPa (138 ksi).

Which condition does FabDigit quote by default, CD or N?

QT-JIS is the default SNCM447 condition in the FabDigit quote flow (neither CD nor N). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, SNCM447-CD or SNCM447-N?

SNCM447-CD, by a small margin. Both rate fair for machinability — 52/100 against 45/100 for SNCM447-N.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SNCM447-CD and SNCM447-N side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.