FabDigitFabDigit

Steel SNCM420-CD vs SNCM420-HR

Steel · SNCM420 temper comparison

SNCM420-CD and SNCM420-HR are two conditions of the same steel grade, SNCM420: CD (cold drawn) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. SNCM420-CD is the stronger of the two: yield strength 660 MPa (95.7 ksi) against 570 MPa (82.7 ksi) for SNCM420-HR, about 16% more. In exchange, SNCM420-HR is the more ductile: elongation 16% versus 12% for SNCM420-CD. On the shop floor, SNCM420-CD machines more easily (good vs fair).

SNCM420-CDChoose it when strength drives the design, or when the part is machined in volume.

SNCM420-HRChoose it when the part is bent, formed or impact-loaded.

SNCM420-CD vs SNCM420-HR: properties

SNCM420-CDSNCM420-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

820 MPa119 ksi
870 MPa126 ksi

Yield Strength (0.2% offset)

660 MPa95.7 ksi
570 MPa82.7 ksi

Elongation at Break

12%
16%

Compressive Strength

680 MPa98.6 ksi
575 MPa83.4 ksi

Shear Strength

490 MPa71.1 ksi
520 MPa75.4 ksi

Fatigue Strength (Endurance Limit)

360 MPa52.2 ksi
385 MPa55.8 ksi

Fracture Toughness (K_IC)

90 MPa·√m81.9 ksi·√in
95 MPa·√m86.5 ksi·√in

Charpy V-Notch Impact (RT)

33 J24.3 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

240 HB
250 HB

Hardness, Rockwell B

99 HRB
100 HRB

Hardness, Vickers

252 HV
263 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Reduction in Area 45%

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,490°C2,714 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 38 W/m·K22 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 250°C482 °F · Min Service Temperature -60°C-76 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7.5 % IACS · Electrical Resistivity 2.3×10⁻⁷ Ω·m9.06 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.65 V · Corrosion Resistance 13 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

65 / 100
50 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
50%

Weldability

33 / 100
35 / 100

Formability (cold)

30 / 100
35 / 100

Same in both: Brazeability / Solderability 55 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 32 MJ/kg13,758 BTU/lb · Embodied Carbon (primary production) 2.3 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSNCM420

SNCM420-CD vs SNCM420-HR — frequently asked

Is SNCM420-CD stronger than SNCM420-HR?

Yes. SNCM420-CD has a typical yield strength of 660 MPa (95.7 ksi) against 570 MPa (82.7 ksi) for SNCM420-HR — about 16% more. Tensile strength is 820 MPa (119 ksi) vs 870 MPa (126 ksi).

Which condition does FabDigit quote by default, CD or HR?

A is the default SNCM420 condition in the FabDigit quote flow (neither CD nor HR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, SNCM420-CD or SNCM420-HR?

SNCM420-CD. Its machinability rates good (65/100) against fair (50/100) for SNCM420-HR.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SNCM420-CD and SNCM420-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.