Steel S355N-CD vs S355N-NL

Steel · S355N temper comparison

S355N-CD and S355N-NL are two conditions of the same steel grade, S355N: CD (cold drawn) versus NL (S355NL). The chemistry is identical, so every difference below comes from the condition. S355N-CD is the stronger of the two: yield strength 470 MPa (68.2 ksi) against 380 MPa (55.1 ksi) for S355N-NL, about 24% more; tensile strength follows at 590 MPa (85.6 ksi) vs 540 MPa (78.3 ksi). In exchange, S355N-NL is the more ductile: elongation 25% versus 14% for S355N-CD, and S355N-CD is harder (185 HB vs 155 HB). S355N-NL runs hotter in service (400°C vs 300°C continuous).

S355N-CDChoose it when strength drives the design.

S355N-NLChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

S355N-CD vs S355N-NL: properties

S355N-CDS355N-NL

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

590 MPa85.6 ksi
540 MPa78.3 ksi

Yield Strength (0.2% offset)

470 MPa68.2 ksi
380 MPa55.1 ksi

Elongation at Break

14%
25%

Reduction in Area

45%
56%

Compressive Strength

470 MPa68.2 ksi
380 MPa55.1 ksi

Shear Strength

360 MPa52.2 ksi
330 MPa47.9 ksi

Fatigue Strength (Endurance Limit)

265 MPa38.4 ksi
245 MPa35.5 ksi

Fracture Toughness (K_IC)

105 MPa·√m95.6 ksi·√in
145 MPa·√m132 ksi·√in

Charpy V-Notch Impact (RT)

60 J44.3 ft·lbf
140 J103 ft·lbf

Hardness, Brinell

185 HB
155 HB

Hardness, Rockwell B

90 HRB
82 HRB

Hardness, Vickers

195 HV
163 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

300°C572 °F
400°C752 °F

Min Service Temperature

-20°C-4 °F
-50°C-58 °F

Same in both: Thermal Conductivity 45 W/m·K26 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 247 J/g106 BTU/lb

Electrical

Conductivity and insulation.

Electrical Conductivity

10.5 % IACS
10.8 % IACS

Electrical Resistivity

1.65×10⁻⁷ Ω·m6.5 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

63 / 100
58 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
60%

Weldability

84 / 100
90 / 100

Formability (cold)

45 / 100
66 / 100

Same in both: Brazeability / Solderability 60 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleS355N

S355N-CD vs S355N-NL — frequently asked

Is S355N-CD stronger than S355N-NL?

Yes. S355N-CD has a typical yield strength of 470 MPa (68.2 ksi) against 380 MPa (55.1 ksi) for S355N-NL — about 24% more. Tensile strength is 590 MPa (85.6 ksi) vs 540 MPa (78.3 ksi).

Which condition does FabDigit quote by default, CD or NL?

+N t<=16 is the default S355N condition in the FabDigit quote flow (neither CD nor NL). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, S355N-CD or S355N-NL?

S355N-CD, by a small margin. Both rate good for machinability — 63/100 against 58/100 for S355N-NL; for welding the order is S355N-NL first (excellent, 90/100) then S355N-CD (very good, 84/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in S355N-CD and S355N-NL side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.