FabDigitFabDigit

Steel S355J0W-CR vs S355J0W +M

Steel · S355J0W temper comparison

S355J0W-CR and S355J0W +M are two conditions of the same steel grade, S355J0W: CR (cold rolled) versus +M (thermomechanically controlled processed). The chemistry is identical, so every difference below comes from the condition. S355J0W +M is the stronger of the two: yield strength 405 MPa (58.7 ksi) against 380 MPa (55.1 ksi) for S355J0W-CR, about 7% more.

S355J0W +MChoose it when strength drives the design.

S355J0W-CR vs S355J0W +M: properties

S355J0W-CRS355J0W +M

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

510 MPa74 ksi
520 MPa75.4 ksi

Yield Strength (0.2% offset)

380 MPa55.1 ksi
405 MPa58.7 ksi

Elongation at Break

24%
26%

Reduction in Area

52%
60%

Compressive Strength

380 MPa55.1 ksi
405 MPa58.7 ksi

Shear Strength

320 MPa46.4 ksi
325 MPa47.1 ksi

Fatigue Strength (Endurance Limit)

240 MPa34.8 ksi
255 MPa37 ksi

Fracture Toughness (K_IC)

100 MPa·√m91 ksi·√in
130 MPa·√m118 ksi·√in

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
120 J88.5 ft·lbf

Hardness, Brinell

160 HB
155 HB

Hardness, Rockwell B

84 HRB
82 HRB

Hardness, Vickers

168 HV
163 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

45 W/m·K26 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 350°C662 °F · Min Service Temperature 0°C32 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8 % IACS · Electrical Resistivity 2.1×10⁻⁷ Ω·m8.27 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 30 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

50 / 100
52 / 100

Machinability Rating (AISI 1212 = 100 %)

56%
58%

Weldability

76 / 100
84 / 100

Polishability

55 / 100
45 / 100

Same in both: Formability (cold) 68 / 100 · Brazeability / Solderability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleS355J0W

S355J0W-CR vs S355J0W +M — frequently asked

Is S355J0W +M stronger than S355J0W-CR?

Yes. S355J0W +M has a typical yield strength of 405 MPa (58.7 ksi) against 380 MPa (55.1 ksi) for S355J0W-CR — about 7% more. Tensile strength is 520 MPa (75.4 ksi) vs 510 MPa (74 ksi).

Which condition does FabDigit quote by default, CR or +M?

+AR is the default S355J0W condition in the FabDigit quote flow (neither CR nor +M). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, S355J0W-CR or S355J0W +M?

S355J0W +M. Its weldability rates very good (84/100) against very good (76/100) for S355J0W-CR.

Ready to make it?

Upload a CAD file and FabDigit prices the part in S355J0W-CR and S355J0W +M side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.