QP1180-CR and QP1180-PB are two conditions of the same steel grade, QP1180: CR (cold rolled) versus PB (formed + paint baked). The chemistry is identical, so every difference below comes from the condition. QP1180-PB is the stronger of the two: yield strength 1,010 MPa (146 ksi) against 920 MPa (133 ksi) for QP1180-CR, about 10% more. In exchange, QP1180-CR is the more ductile: elongation 15% versus 11% for QP1180-PB.

QP1180-CRChoose it when the part is bent, formed or impact-loaded.

QP1180-PBChoose it when strength drives the design.

QP1180-CR vs QP1180-PB: properties

QP1180-CRQP1180-PB

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

1,240 MPa180 ksi
1,290 MPa187 ksi

Yield Strength (0.2% offset)

920 MPa133 ksi
1,010 MPa146 ksi

Elongation at Break

15%
11%

Shear Strength

740 MPa107 ksi
770 MPa112 ksi

Fatigue Strength (Endurance Limit)

540 MPa78.3 ksi
560 MPa81.2 ksi

Fracture Toughness (K_IC)

50 MPa·√m45.5 ksi·√in
45 MPa·√m41 ksi·√in

Hardness, Brinell

360 HB
372 HB

Hardness, Rockwell C

39 HRC
40 HRC

Hardness, Vickers

380 HV
395 HV

Same in both: Elastic (Young's) Modulus 207 GPa30 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 165 GPa23.9 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,450°C2,642 °F · Liquidus Temperature 1,505°C2,741 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 28 W/m·K16.2 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.5 µm/m·K6.9 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 3.8 % IACS · Electrical Resistivity 4.5×10⁻⁷ Ω·m17.7 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

22 / 100
20 / 100

Machinability Rating (AISI 1212 = 100 %)

22%
20%

Weldability

60 / 100
52 / 100

Formability (cold)

47 / 100
30 / 100

Same in both: Brazeability / Solderability 35 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 32 MJ/kg13,758 BTU/lb · Embodied Carbon (primary production) 2.4 kg CO₂/kg · Embodied Water 50 L/kg6 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleQP1180

QP1180-CR vs QP1180-PB — frequently asked

Is QP1180-PB stronger than QP1180-CR?

Yes. QP1180-PB has a typical yield strength of 1,010 MPa (146 ksi) against 920 MPa (133 ksi) for QP1180-CR — about 10% more. Tensile strength is 1,290 MPa (187 ksi) vs 1,240 MPa (180 ksi).

Which condition does FabDigit quote by default, CR or PB?

CR is the default QP1180 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, QP1180-CR or QP1180-PB?

QP1180-CR. Its weldability rates good (60/100) against fair (52/100) for QP1180-PB.