FabDigitFabDigit

Steel P690QL2-QT vs P690QL2 QT-50-100

Steel · P690QL2 temper comparison

P690QL2-QT and P690QL2 QT-50-100 are two conditions of the same steel grade, P690QL2: QT (quenched and tempered) versus QT-50-100 (QT). The chemistry is identical, so every difference below comes from the condition. P690QL2-QT is the stronger of the two: yield strength 750 MPa (109 ksi) against 710 MPa (103 ksi) for P690QL2 QT-50-100, about 6% more. P690QL2-QT is harder — 25 HRC against 23 HRC for P690QL2 QT-50-100 — which matters for wear surfaces and threads.

P690QL2-QTChoose it when strength drives the design, or when surface hardness matters.

P690QL2-QT vs P690QL2 QT-50-100: properties

P690QL2-QTP690QL2 QT-50-100

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

840 MPa122 ksi
830 MPa120 ksi

Yield Strength (0.2% offset)

750 MPa109 ksi
710 MPa103 ksi

Compressive Strength

750 MPa109 ksi
710 MPa103 ksi

Shear Strength

520 MPa75.4 ksi
505 MPa73.2 ksi

Fatigue Strength (Endurance Limit)

380 MPa55.1 ksi
370 MPa53.7 ksi

Fracture Toughness (K_IC)

130 MPa·√m118 ksi·√in
125 MPa·√m114 ksi·√in

Charpy V-Notch Impact (RT)

150 J111 ft·lbf
130 J95.9 ft·lbf

Hardness, Brinell

255 HB
245 HB

Hardness, Rockwell C

25 HRC
23 HRC

Hardness, Vickers

268 HV
257 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3 · Elongation at Break 18% · Reduction in Area 55%

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,430°C2,606 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 38 W/m·K22 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.5 µm/m·K6.9 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -60°C-76 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Resistivity 2.5×10⁻⁷ Ω·m9.84 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

35 / 100
37 / 100

Machinability Rating (AISI 1212 = 100 %)

40%
42%

Weldability

60 / 100
58 / 100

Formability (cold)

40 / 100
35 / 100

Same in both: Polishability 50 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.3 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleP690QL2

P690QL2-QT vs P690QL2 QT-50-100 — frequently asked

Is P690QL2-QT stronger than P690QL2 QT-50-100?

Yes. P690QL2-QT has a typical yield strength of 750 MPa (109 ksi) against 710 MPa (103 ksi) for P690QL2 QT-50-100 — about 6% more. Tensile strength is 840 MPa (122 ksi) vs 830 MPa (120 ksi).

Which condition does FabDigit quote by default, QT or QT-50-100?

QT is the default P690QL2 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose P690QL2-QT over P690QL2 QT-50-100?

Pick P690QL2-QT when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in P690QL2-QT and P690QL2 QT-50-100 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.