FabDigitFabDigit

Steel P355NL1-N vs P355NL1 N-50-70

Steel · P355NL1 temper comparison

P355NL1-N and P355NL1 N-50-70 are two conditions of the same steel grade, P355NL1: N (normalized) versus N-50-70 (n). The chemistry is identical, so every difference below comes from the condition. P355NL1-N is the stronger of the two: yield strength 390 MPa (56.6 ksi) against 360 MPa (52.2 ksi) for P355NL1 N-50-70, about 8% more.

P355NL1-NChoose it when strength drives the design.

P355NL1-N vs P355NL1 N-50-70: properties

P355NL1-NP355NL1 N-50-70

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

550 MPa79.8 ksi
535 MPa77.6 ksi

Yield Strength (0.2% offset)

390 MPa56.6 ksi
360 MPa52.2 ksi

Elongation at Break

28%
27%

Reduction in Area

60%
58%

Compressive Strength

390 MPa56.6 ksi
360 MPa52.2 ksi

Shear Strength

340 MPa49.3 ksi
330 MPa47.9 ksi

Fatigue Strength (Endurance Limit)

245 MPa35.5 ksi
233 MPa33.8 ksi

Fracture Toughness (K_IC)

130 MPa·√m118 ksi·√in
122 MPa·√m111 ksi·√in

Charpy V-Notch Impact (RT)

180 J133 ft·lbf
150 J111 ft·lbf

Hardness, Brinell

155 HB
148 HB

Hardness, Rockwell B

81 HRB
78 HRB

Hardness, Vickers

163 HV
156 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 45 W/m·K26 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 260 J/g112 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8.6 % IACS · Electrical Resistivity 2×10⁻⁷ Ω·m7.87 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.65 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
57 / 100

Machinability Rating (AISI 1212 = 100 %)

62%
64%

Weldability

88 / 100
86 / 100

Formability (cold)

68 / 100
64 / 100

Same in both: Brazeability / Solderability 55 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 28%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleP355NL1

P355NL1-N vs P355NL1 N-50-70 — frequently asked

Is P355NL1-N stronger than P355NL1 N-50-70?

Yes. P355NL1-N has a typical yield strength of 390 MPa (56.6 ksi) against 360 MPa (52.2 ksi) for P355NL1 N-50-70 — about 8% more. Tensile strength is 550 MPa (79.8 ksi) vs 535 MPa (77.6 ksi).

Which condition does FabDigit quote by default, N or N-50-70?

N is the default P355NL1 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose P355NL1-N over P355NL1 N-50-70?

Pick P355NL1-N when strength drives the design.

Ready to make it?

Upload a CAD file and FabDigit prices the part in P355NL1-N and P355NL1 N-50-70 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.