FabDigitFabDigit

Steel P265TR1 +A vs P265TR1 +N

Steel · P265TR1 temper comparison

P265TR1 +A and P265TR1 +N are two conditions of the same steel grade, P265TR1: +A (annealed) versus +N (normalized). The chemistry is identical, so every difference below comes from the condition. P265TR1 +N is the stronger of the two: yield strength 295 MPa (42.8 ksi) against 260 MPa (37.7 ksi) for P265TR1 +A, about 13% more; tensile strength follows at 460 MPa (66.7 ksi) vs 420 MPa (60.9 ksi). P265TR1 +N is harder — 125 HB against 115 HB for P265TR1 +A — which matters for wear surfaces and threads.

P265TR1 +NChoose it when strength drives the design, or when surface hardness matters.

P265TR1 +A vs P265TR1 +N: properties

P265TR1 +AP265TR1 +N

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

420 MPa60.9 ksi
460 MPa66.7 ksi

Yield Strength (0.2% offset)

260 MPa37.7 ksi
295 MPa42.8 ksi

Elongation at Break

30%
28%

Reduction in Area

62%
55%

Compressive Strength

260 MPa37.7 ksi
300 MPa43.5 ksi

Shear Strength

270 MPa39.2 ksi
300 MPa43.5 ksi

Fatigue Strength (Endurance Limit)

195 MPa28.3 ksi
210 MPa30.5 ksi

Fracture Toughness (K_IC)

130 MPa·√m118 ksi·√in
120 MPa·√m109 ksi·√in

Charpy V-Notch Impact (RT)

55 J40.6 ft·lbf
60 J44.3 ft·lbf

Hardness, Brinell

115 HB
125 HB

Hardness, Rockwell B

64 HRB
70 HRB

Hardness, Vickers

121 HV
137 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,460°C2,660 °F · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

51 W/m·K29.5 BTU/hr·ft·°F
50 W/m·K28.9 BTU/hr·ft·°F

Min Service Temperature

-10°C14 °F
-20°C-4 °F

Same in both: Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 247 J/g106 BTU/lb · Max Service Temperature (continuous) 300°C572 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

56 / 100
60 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
72%

Weldability

93 / 100
92 / 100

Formability (cold)

88 / 100
82 / 100

Same in both: Brazeability / Solderability 70 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleP265TR1

P265TR1 +A vs P265TR1 +N — frequently asked

Is P265TR1 +N stronger than P265TR1 +A?

Yes. P265TR1 +N has a typical yield strength of 295 MPa (42.8 ksi) against 260 MPa (37.7 ksi) for P265TR1 +A — about 13% more. Tensile strength is 460 MPa (66.7 ksi) vs 420 MPa (60.9 ksi).

Which condition does FabDigit quote by default, +A or +N?

AR is the default P265TR1 condition in the FabDigit quote flow (neither +A nor +N). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose P265TR1 +A over P265TR1 +N?

Pick P265TR1 +N when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in P265TR1 +A and P265TR1 +N side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.