GS200-N and GS200-SR are two conditions of the same steel grade, GS200: N (normalized) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. GS200-N is the stronger of the two: yield strength 220 MPa (31.9 ksi) against 200 MPa (29 ksi) for GS200-SR, about 10% more; tensile strength follows at 430 MPa (62.4 ksi) vs 405 MPa (58.7 ksi). GS200-N is harder — 125 HB against 118 HB for GS200-SR — which matters for wear surfaces and threads.

GS200-NChoose it when strength drives the design, or when surface hardness matters.

GS200-N vs GS200-SR: properties

GS200-NGS200-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

430 MPa62.4 ksi
405 MPa58.7 ksi

Yield Strength (0.2% offset)

220 MPa31.9 ksi
200 MPa29 ksi

Elongation at Break

25%
23%

Reduction in Area

40%
38%

Compressive Strength

220 MPa31.9 ksi
200 MPa29 ksi

Shear Strength

280 MPa40.6 ksi
262 MPa38 ksi

Fatigue Strength (Endurance Limit)

180 MPa26.1 ksi
162 MPa23.5 ksi

Fracture Toughness (K_IC)

100 MPa·√m91 ksi·√in
92 MPa·√m83.7 ksi·√in

Charpy V-Notch Impact (RT)

35 J25.8 ft·lbf
28 J20.7 ft·lbf

Hardness, Brinell

125 HB
118 HB

Hardness, Rockwell B

70 HRB
66 HRB

Hardness, Vickers

130 HV
124 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 50 W/m·K28.9 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 425°C797 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
63 / 100

Machinability Rating (AISI 1212 = 100 %)

68%
67%

Same in both: Weldability 88 / 100 · Formability (cold) 25 / 100 · Castability 78 / 100 · Brazeability / Solderability 70 / 100 · Polishability 50 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 85%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleGS200

GS200-N vs GS200-SR — frequently asked

Is GS200-N stronger than GS200-SR?

Yes. GS200-N has a typical yield strength of 220 MPa (31.9 ksi) against 200 MPa (29 ksi) for GS200-SR — about 10% more. Tensile strength is 430 MPa (62.4 ksi) vs 405 MPa (58.7 ksi).

Which condition does FabDigit quote by default, N or SR?

N is the default GS200 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose GS200-N over GS200-SR?

Pick GS200-N when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in GS200-N and GS200-SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.