E590-AR and E590-N are two conditions of the same steel grade, E590: AR versus N (normalized). The chemistry is identical, so every difference below comes from the condition. Both yield at about 610 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (AR versus normalized). E590-N is the more ductile: elongation 19% versus 17% for E590-AR.

E590-NChoose it when the part is bent, formed or impact-loaded.

E590-AR vs E590-N: properties

E590-ARE590-N

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Yield Strength (0.2% offset)

610 MPa88.5 ksi
615 MPa89.2 ksi

Elongation at Break

17%
19%

Reduction in Area

48%
52%

Compressive Strength

610 MPa88.5 ksi
615 MPa89.2 ksi

Fatigue Strength (Endurance Limit)

340 MPa49.3 ksi
345 MPa50 ksi

Fracture Toughness (K_IC)

80 MPa·√m72.8 ksi·√in
100 MPa·√m91 ksi·√in

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
70 J51.6 ft·lbf

Hardness, Rockwell B

99 HRB
98 HRB

Hardness, Rockwell C

21 HRC
20 HRC

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Tensile Strength (Ultimate) 780 MPa113 ksi · Shear Strength 470 MPa68.2 ksi · Hardness, Brinell 230 HB · Hardness, Vickers 240 HV

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 45 W/m·K26 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 350°C662 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 9.5 % IACS · Electrical Resistivity 1.8×10⁻⁷ Ω·m7.09 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Weldability

53 / 100
60 / 100

Formability (cold)

40 / 100
45 / 100

Same in both: Machinability 47 / 100 · Machinability Rating (AISI 1212 = 100 %) 52% · Brazeability / Solderability 40 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleE590

E590-AR vs E590-N — frequently asked

What is the difference between E590-AR and E590-N?

E590-AR and E590-N are two conditions of the same steel grade, E590: AR versus N (normalized). The chemistry is identical, so every difference below comes from the condition. Both yield at about 610 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (AR versus normalized).

Which condition does FabDigit quote by default, AR or N?

QT is the default E590 condition in the FabDigit quote flow (neither AR nor N). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, E590-AR or E590-N?

E590-N. Its weldability rates good (60/100) against fair (53/100) for E590-AR.