Steel DP450-CR vs DP450 +ZF

Steel · DP450 temper comparison

DP450-CR and DP450 +ZF are two conditions of the same steel grade, DP450: CR (cold rolled) versus +ZF (galvannealed). The chemistry is identical, so every difference below comes from the condition. Both yield at about 300 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (cold rolled versus galvannealed). DP450 +ZF runs hotter in service (250°C vs 200°C continuous).

DP450 +ZFChoose it when the part sees heat.

DP450-CR vs DP450 +ZF: properties

DP450-CRDP450 +ZF

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Yield Strength (0.2% offset)

300 MPa43.5 ksi
310 MPa45 ksi

Elongation at Break

29%
27%

Fatigue Strength (Endurance Limit)

250 MPa36.3 ksi
240 MPa34.8 ksi

Hardness, Brinell

143 HB
146 HB

Hardness, Rockwell B

80 HRB
81 HRB

Hardness, Vickers

150 HV
152 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 165 GPa23.9 Msi · Poisson's Ratio 0.3 · Tensile Strength (Ultimate) 500 MPa72.5 ksi · Shear Strength 330 MPa47.9 ksi

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,480°C2,696 °F · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

200°C392 °F
250°C482 °F

Same in both: Thermal Conductivity 48 W/m·K27.7 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

9.1 % IACS
9 % IACS

Same in both: Electrical Resistivity 1.9×10⁻⁷ Ω·m7.48 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

12 / 100
30 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.65 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
50 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
60%

Weldability

82 / 100
78 / 100

Formability (cold)

75 / 100
68 / 100

Same in both: Brazeability / Solderability 60 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.3 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleDP450

DP450-CR vs DP450 +ZF — frequently asked

What is the difference between DP450-CR and DP450 +ZF?

DP450-CR and DP450 +ZF are two conditions of the same steel grade, DP450: CR (cold rolled) versus +ZF (galvannealed). The chemistry is identical, so every difference below comes from the condition. Both yield at about 300 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (cold rolled versus galvannealed).

Which condition does FabDigit quote by default, CR or +ZF?

CR is the default DP450 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, DP450-CR or DP450 +ZF?

DP450-CR. Its machinability rates good (55/100) against fair (50/100) for DP450 +ZF.

Ready to make it?

Upload a CAD file and FabDigit prices the part in DP450-CR and DP450 +ZF side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.