FabDigitFabDigit

Steel DP1470-BH vs DP1470-CR

Steel · DP1470 temper comparison

DP1470-BH and DP1470-CR are two conditions of the same steel grade, DP1470: BH (after 2 % prestrain + paint bake) versus CR (cold rolled). The chemistry is identical, so every difference below comes from the condition. DP1470-BH is the stronger of the two: yield strength 1,240 MPa (180 ksi) against 1,120 MPa (162 ksi) for DP1470-CR, about 11% more. In exchange, DP1470-CR is the more ductile: elongation 5.5% versus 3.5% for DP1470-BH.

DP1470-BHChoose it when strength drives the design.

DP1470-CRChoose it when the part is bent, formed or impact-loaded.

DP1470-BH vs DP1470-CR: properties

DP1470-BHDP1470-CR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

205 GPa29.7 Msi
207 GPa30 Msi

Tensile Strength (Ultimate)

1,560 MPa226 ksi
1,520 MPa220 ksi

Yield Strength (0.2% offset)

1,240 MPa180 ksi
1,120 MPa162 ksi

Elongation at Break

3.5%
5.5%

Compressive Strength

1,560 MPa226 ksi
1,150 MPa167 ksi

Shear Strength

970 MPa141 ksi
950 MPa138 ksi

Fatigue Strength (Endurance Limit)

615 MPa89.2 ksi
600 MPa87 ksi

Charpy V-Notch Impact (RT)

8 J5.9 ft·lbf
12 J8.9 ft·lbf

Hardness, Brinell

437 HB
430 HB

Hardness, Rockwell C

46 HRC
45 HRC

Hardness, Vickers

460 HV
450 HV

Same in both: Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3 · Reduction in Area 30% · Fracture Toughness (K_IC) 45 MPa·√m41 ksi·√in

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,450°C2,642 °F · Liquidus Temperature 1,505°C2,741 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 42 W/m·K24.3 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.5 µm/m·K6.9 µin/in·°F · Latent Heat of Fusion 247 J/g106 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8.5 % IACS · Electrical Resistivity 2×10⁻⁷ Ω·m7.87 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

16 / 100
18 / 100

Machinability Rating (AISI 1212 = 100 %)

22%
25%

Weldability

48 / 100
52 / 100

Formability (cold)

12 / 100
18 / 100

Same in both: Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 32 MJ/kg13,758 BTU/lb · Embodied Carbon (primary production) 2.4 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 20%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleDP1470

DP1470-BH vs DP1470-CR — frequently asked

Is DP1470-BH stronger than DP1470-CR?

Yes. DP1470-BH has a typical yield strength of 1,240 MPa (180 ksi) against 1,120 MPa (162 ksi) for DP1470-CR — about 11% more. Tensile strength is 1,560 MPa (226 ksi) vs 1,520 MPa (220 ksi).

Which condition does FabDigit quote by default, BH or CR?

CR is the default DP1470 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose DP1470-BH over DP1470-CR?

Pick DP1470-BH when strength drives the design. Pick DP1470-CR when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in DP1470-BH and DP1470-CR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.