A588-CR and A588-N are two conditions of the same steel grade, A588: CR (cold rolled) versus N (normalized). The chemistry is identical, so every difference below comes from the condition. A588-N is the stronger of the two: tensile strength 530 MPa (76.9 ksi) against 500 MPa (72.5 ksi) for A588-CR, about 6% more. A588-N is the more ductile: elongation 27% versus 22% for A588-CR, and A588-CR is harder (160 HB vs 150 HB).

A588-NChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

A588-CR vs A588-N: properties

A588-CRA588-N

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

500 MPa72.5 ksi
530 MPa76.9 ksi

Yield Strength (0.2% offset)

380 MPa55.1 ksi
390 MPa56.6 ksi

Elongation at Break

22%
27%

Reduction in Area

40%
52%

Compressive Strength

380 MPa55.1 ksi
390 MPa56.6 ksi

Shear Strength

310 MPa45 ksi
330 MPa47.9 ksi

Fatigue Strength (Endurance Limit)

230 MPa33.4 ksi
245 MPa35.5 ksi

Fracture Toughness (K_IC)

120 MPa·√m109 ksi·√in
150 MPa·√m137 ksi·√in

Charpy V-Notch Impact (RT)

40 J29.5 ft·lbf
95 J70.1 ft·lbf

Hardness, Brinell

160 HB
150 HB

Hardness, Rockwell B

85 HRB
80 HRB

Hardness, Vickers

168 HV
157 HV

Same in both: Elastic (Young's) Modulus 200 GPa29 Msi · Shear Modulus 79 GPa11.5 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,490°C2,714 °F · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Min Service Temperature

-40°C-40 °F
-50°C-58 °F

Same in both: Thermal Conductivity 52 W/m·K30 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8.6 % IACS · Electrical Resistivity 2×10⁻⁷ Ω·m7.87 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.65 V · Corrosion Resistance 32 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

52 / 100
57 / 100

Machinability Rating (AISI 1212 = 100 %)

55%
60%

Weldability

76 / 100
80 / 100

Formability (cold)

65 / 100
62 / 100

Polishability

50 / 100
45 / 100

Same in both: Brazeability / Solderability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleA588

A588-CR vs A588-N — frequently asked

Is A588-N stronger than A588-CR?

Yes. A588-N has a typical tensile strength of 530 MPa (76.9 ksi) against 500 MPa (72.5 ksi) for A588-CR — about 6% more.

Which condition does FabDigit quote by default, CR or N?

HR is the default A588 condition in the FabDigit quote flow (neither CR nor N). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, A588-CR or A588-N?

A588-N. Its machinability rates good (57/100) against fair (52/100) for A588-CR.