FabDigitFabDigit

Steel A369 FP1-ANN vs A369 FP1-NT

Steel · A369 FP1 temper comparison

A369 FP1-ANN and A369 FP1-NT are two conditions of the same steel grade, A369 FP1: ANN (annealed) versus NT (normalized and Tempered). The chemistry is identical, so every difference below comes from the condition. A369 FP1-NT is the stronger of the two: yield strength 300 MPa (43.5 ksi) against 270 MPa (39.2 ksi) for A369 FP1-ANN, about 11% more. A369 FP1-NT is harder — 150 HB against 140 HB for A369 FP1-ANN — which matters for wear surfaces and threads.

A369 FP1-NTChoose it when strength drives the design, or when surface hardness matters.

A369 FP1-ANN vs A369 FP1-NT: properties

A369 FP1-ANNA369 FP1-NT

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

460 MPa66.7 ksi
480 MPa69.6 ksi

Yield Strength (0.2% offset)

270 MPa39.2 ksi
300 MPa43.5 ksi

Elongation at Break

34%
32%

Fatigue Strength (Endurance Limit)

215 MPa31.2 ksi
230 MPa33.4 ksi

Fracture Toughness (K_IC)

110 MPa·√m100 ksi·√in
120 MPa·√m109 ksi·√in

Charpy V-Notch Impact (RT)

85 J62.7 ft·lbf
110 J81.1 ft·lbf

Hardness, Brinell

140 HB
150 HB

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Reduction in Area 62% · Compressive Strength 280 MPa40.6 ksi · Shear Strength 300 MPa43.5 ksi · Hardness, Rockwell B 78 HRB

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,470°C2,678 °F · Liquidus Temperature 1,515°C2,759 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

470°C878 °F
500°C932 °F

Same in both: Thermal Conductivity 44 W/m·K25.4 BTU/hr·ft·°F · Specific Heat Capacity 465 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.2 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Min Service Temperature -29°C-20 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Resistivity 2.1×10⁻⁷ Ω·m8.27 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Corrosion Resistance 13 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

60 / 100
57 / 100

Machinability Rating (AISI 1212 = 100 %)

62%
58%

Weldability

72 / 100
70 / 100

Formability (cold)

70 / 100
65 / 100

Same in both: Brazeability / Solderability 45 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.3 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleA369 FP1

A369 FP1-ANN vs A369 FP1-NT — frequently asked

Is A369 FP1-NT stronger than A369 FP1-ANN?

Yes. A369 FP1-NT has a typical yield strength of 300 MPa (43.5 ksi) against 270 MPa (39.2 ksi) for A369 FP1-ANN — about 11% more. Tensile strength is 480 MPa (69.6 ksi) vs 460 MPa (66.7 ksi).

Which condition does FabDigit quote by default, ANN or NT?

ANN is the default A369 FP1 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose A369 FP1-ANN over A369 FP1-NT?

Pick A369 FP1-NT when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in A369 FP1-ANN and A369 FP1-NT side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.