FabDigitFabDigit

Steel A283-HR vs A283 Normalized

Steel · A283 temper comparison

A283-HR and A283 Normalized are two conditions of the same steel grade, A283: HR (hot rolled) versus Normalized. The chemistry is identical, so every difference below comes from the condition. Both yield at about 230 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (hot rolled versus Normalized). A283 Normalized is the more ductile: elongation 28% versus 25% for A283-HR.

A283 NormalizedChoose it when the part is bent, formed or impact-loaded.

A283-HR vs A283 Normalized: properties

A283-HRA283 Normalized

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

420 MPa60.9 ksi
425 MPa61.6 ksi

Yield Strength (0.2% offset)

230 MPa33.4 ksi
240 MPa34.8 ksi

Elongation at Break

25%
28%

Reduction in Area

45%
48%

Compressive Strength

230 MPa33.4 ksi
240 MPa34.8 ksi

Shear Strength

270 MPa39.2 ksi
275 MPa39.9 ksi

Fatigue Strength (Endurance Limit)

190 MPa27.6 ksi
200 MPa29 ksi

Fracture Toughness (K_IC)

90 MPa·√m81.9 ksi·√in
110 MPa·√m100 ksi·√in

Charpy V-Notch Impact (RT)

27 J19.9 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

120 HB
125 HB

Hardness, Rockwell B

68 HRB
71 HRB

Hardness, Vickers

126 HV
131 HV

Same in both: Elastic (Young's) Modulus 200 GPa29 Msi · Shear Modulus 79 GPa11.5 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

400°C752 °F
425°C797 °F

Same in both: Thermal Conductivity 51 W/m·K29.5 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 247 J/g106 BTU/lb · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10.8 % IACS · Electrical Resistivity 1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.65 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

65 / 100
64 / 100

Machinability Rating (AISI 1212 = 100 %)

70%
68%

Same in both: Weldability 95 / 100 · Formability (cold) 78 / 100 · Brazeability / Solderability 70 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 1.9 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleA283

A283-HR vs A283 Normalized — frequently asked

What is the difference between A283-HR and A283 Normalized?

A283-HR and A283 Normalized are two conditions of the same steel grade, A283: HR (hot rolled) versus Normalized. The chemistry is identical, so every difference below comes from the condition. Both yield at about 230 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (hot rolled versus Normalized).

Which condition does FabDigit quote by default, HR or Normalized?

HR is the default A283 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose A283-HR over A283 Normalized?

Pick A283 Normalized when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in A283-HR and A283 Normalized side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.