FabDigitFabDigit

Steel 60#-CD vs 60# Normalized

Steel · 60# temper comparison

60#-CD and 60# Normalized are two conditions of the same steel grade, 60#: CD (cold drawn) versus Normalized. The chemistry is identical, so every difference below comes from the condition. 60#-CD is the stronger of the two: yield strength 660 MPa (95.7 ksi) against 430 MPa (62.4 ksi) for 60# Normalized, about 53% more; tensile strength follows at 830 MPa (120 ksi) vs 730 MPa (106 ksi). In exchange, 60# Normalized is the more ductile: elongation 17% versus 9% for 60#-CD.

60#-CDChoose it when strength drives the design.

60# NormalizedChoose it when the part is bent, formed or impact-loaded.

60#-CD vs 60# Normalized: properties

60#-CD60# Normalized

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

830 MPa120 ksi
730 MPa106 ksi

Yield Strength (0.2% offset)

660 MPa95.7 ksi
430 MPa62.4 ksi

Elongation at Break

9%
17%

Reduction in Area

30%
38%

Fatigue Strength (Endurance Limit)

360 MPa52.2 ksi
320 MPa46.4 ksi

Charpy V-Notch Impact (RT)

28 J20.7 ft·lbf
22 J16.2 ft·lbf

Hardness, Brinell

250 HB
241 HB

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Shear Strength 460 MPa66.7 ksi · Hardness, Rockwell B 91 HRB

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,470°C2,678 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 48 W/m·K27.7 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

58 / 100
52 / 100

Machinability Rating (AISI 1212 = 100 %)

62%
55%

Formability (cold)

20 / 100
30 / 100

Same in both: Weldability 20 / 100 · Castability 45 / 100 · Brazeability / Solderability 55 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 26 MJ/kg11,178 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale60#

60#-CD vs 60# Normalized — frequently asked

Is 60#-CD stronger than 60# Normalized?

Yes. 60#-CD has a typical yield strength of 660 MPa (95.7 ksi) against 430 MPa (62.4 ksi) for 60# Normalized — about 53% more. Tensile strength is 830 MPa (120 ksi) vs 730 MPa (106 ksi).

Which condition does FabDigit quote by default, CD or Normalized?

Annealed is the default 60# condition in the FabDigit quote flow (neither CD nor Normalized). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, 60#-CD or 60# Normalized?

60#-CD. Its machinability rates good (58/100) against fair (52/100) for 60# Normalized.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 60#-CD and 60# Normalized side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.