FabDigitFabDigit

Steel 50B46-CD vs 50B46-HR

Steel · 50B46 temper comparison

50B46-CD and 50B46-HR are two conditions of the same steel grade, 50B46: CD (cold drawn) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. 50B46-CD is the stronger of the two: yield strength 700 MPa (102 ksi) against 470 MPa (68.2 ksi) for 50B46-HR, about 49% more. In exchange, 50B46-HR is the more ductile: elongation 16% versus 12% for 50B46-CD. 50B46-HR runs hotter in service (350°C vs 300°C continuous).

50B46-CDChoose it when strength drives the design.

50B46-HRChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

50B46-CD vs 50B46-HR: properties

50B46-CD50B46-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

830 MPa120 ksi
800 MPa116 ksi

Yield Strength (0.2% offset)

700 MPa102 ksi
470 MPa68.2 ksi

Elongation at Break

12%
16%

Reduction in Area

35%
38%

Compressive Strength

720 MPa104 ksi
480 MPa69.6 ksi

Shear Strength

500 MPa72.5 ksi
490 MPa71.1 ksi

Fatigue Strength (Endurance Limit)

380 MPa55.1 ksi
370 MPa53.7 ksi

Fracture Toughness (K_IC)

80 MPa·√m72.8 ksi·√in
85 MPa·√m77.4 ksi·√in

Charpy V-Notch Impact (RT)

14 J10.3 ft·lbf
22 J16.2 ft·lbf

Hardness, Brinell

241 HB
229 HB

Hardness, Rockwell B

100 HRB
98 HRB

Hardness, Vickers

253 HV
241 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,490°C2,714 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

300°C572 °F
350°C662 °F

Same in both: Thermal Conductivity 44 W/m·K25.4 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Min Service Temperature -30°C-22 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

58 / 100
50 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
55%

Weldability

28 / 100
30 / 100

Formability (cold)

30 / 100
40 / 100

Same in both: Castability 35 / 100 · Brazeability / Solderability 55 / 100 · Polishability 65 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 29 MJ/kg12,468 BTU/lb · Embodied Carbon (primary production) 2.1 kg CO₂/kg · Embodied Water 50 L/kg6 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale50B46

50B46-CD vs 50B46-HR — frequently asked

Is 50B46-CD stronger than 50B46-HR?

Yes. 50B46-CD has a typical yield strength of 700 MPa (102 ksi) against 470 MPa (68.2 ksi) for 50B46-HR — about 49% more. Tensile strength is 830 MPa (120 ksi) vs 800 MPa (116 ksi).

Which condition does FabDigit quote by default, CD or HR?

A is the default 50B46 condition in the FabDigit quote flow (neither CD nor HR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, 50B46-CD or 50B46-HR?

50B46-CD. Its machinability rates good (58/100) against fair (50/100) for 50B46-HR.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 50B46-CD and 50B46-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.