4720-HR and 4720-N are two conditions of the same steel grade, 4720: HR (hot rolled) versus N (normalized). The chemistry is identical, so every difference below comes from the condition. 4720-N is the stronger of the two: yield strength 430 MPa (62.4 ksi) against 400 MPa (58 ksi) for 4720-HR, about 8% more. 4720-N is harder — 200 HB against 190 HB for 4720-HR — which matters for wear surfaces and threads.

4720-NChoose it when strength drives the design, or when surface hardness matters.

4720-HR vs 4720-N: properties

4720-HR4720-N

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

620 MPa89.9 ksi
640 MPa92.8 ksi

Yield Strength (0.2% offset)

400 MPa58 ksi
430 MPa62.4 ksi

Elongation at Break

22%
23%

Reduction in Area

50%
55%

Compressive Strength

400 MPa58 ksi
430 MPa62.4 ksi

Shear Strength

400 MPa58 ksi
420 MPa60.9 ksi

Fatigue Strength (Endurance Limit)

285 MPa41.3 ksi
300 MPa43.5 ksi

Fracture Toughness (K_IC)

80 MPa·√m72.8 ksi·√in
85 MPa·√m77.4 ksi·√in

Charpy V-Notch Impact (RT)

50 J36.9 ft·lbf
60 J44.3 ft·lbf

Hardness, Brinell

190 HB
200 HB

Hardness, Rockwell B

91 HRB
93 HRB

Hardness, Vickers

199 HV
210 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,500°C2,732 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 43 W/m·K24.8 BTU/hr·ft·°F · Specific Heat Capacity 475 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 350°C662 °F · Min Service Temperature -50°C-58 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7.8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

54 / 100
58 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
65%

Weldability

58 / 100
55 / 100

Formability (cold)

58 / 100
55 / 100

Same in both: Brazeability / Solderability 65 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 31 MJ/kg13,328 BTU/lb · Embodied Carbon (primary production) 2.2 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale4720

4720-HR vs 4720-N — frequently asked

Is 4720-N stronger than 4720-HR?

Yes. 4720-N has a typical yield strength of 430 MPa (62.4 ksi) against 400 MPa (58 ksi) for 4720-HR — about 8% more. Tensile strength is 640 MPa (92.8 ksi) vs 620 MPa (89.9 ksi).

Which condition does FabDigit quote by default, HR or N?

N is the default 4720 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose 4720-HR over 4720-N?

Pick 4720-N when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 4720-HR and 4720-N side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.