FabDigitFabDigit

Steel 4150 Annealed vs 4150-CD

Steel · 4150 temper comparison

4150 Annealed and 4150-CD are two conditions of the same steel grade, 4150: Annealed versus CD (cold drawn). The chemistry is identical, so every difference below comes from the condition. 4150-CD is the stronger of the two: yield strength 830 MPa (120 ksi) against 380 MPa (55.1 ksi) for 4150 Annealed, about 118% more; tensile strength follows at 945 MPa (137 ksi) vs 730 MPa (106 ksi). In exchange, 4150 Annealed is the more ductile: elongation 20% versus 10% for 4150-CD, and 4150-CD is harder (277 HB vs 197 HB).

4150 AnnealedChoose it when the part is bent, formed or impact-loaded.

4150-CDChoose it when strength drives the design.

4150 Annealed vs 4150-CD: properties

4150 Annealed4150-CD

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

730 MPa106 ksi
945 MPa137 ksi

Yield Strength (0.2% offset)

380 MPa55.1 ksi
830 MPa120 ksi

Elongation at Break

20%
10%

Reduction in Area

40%
30%

Shear Strength

560 MPa81.2 ksi
570 MPa82.7 ksi

Fatigue Strength (Endurance Limit)

330 MPa47.9 ksi
440 MPa63.8 ksi

Charpy V-Notch Impact (RT)

27 J19.9 ft·lbf
16 J11.8 ft·lbf

Hardness, Brinell

197 HB
277 HB

Hardness, Rockwell C

21 HRC
28 HRC

Hardness, Vickers

245 HV
291 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Liquidus Temperature

1,490°C2,714 °F
1,471°C2,680 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,416°C2,581 °F

Thermal

How each material carries heat and how hot it can run.

Min Service Temperature

-40°C-40 °F
-25°C-13 °F

Same in both: Thermal Conductivity 42.6 W/m·K24.6 BTU/hr·ft·°F · Specific Heat Capacity 473 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.3 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7.8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
50 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
55%

Weldability

25 / 100
28 / 100

Formability (cold)

40 / 100
18 / 100

Polishability

60 / 100
62 / 100

Same in both: Castability 35 / 100 · Brazeability / Solderability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

31 MJ/kg13,328 BTU/lb
30 MJ/kg12,898 BTU/lb

Embodied Carbon (primary production)

2.3 kg CO₂/kg
2.2 kg CO₂/kg

Typical Recycled Content

30%
25%

Same in both: Embodied Water 60 L/kg7.2 gal/lb

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale4150

4150 Annealed vs 4150-CD — frequently asked

Is 4150-CD stronger than 4150 Annealed?

Yes. 4150-CD has a typical yield strength of 830 MPa (120 ksi) against 380 MPa (55.1 ksi) for 4150 Annealed — about 118% more. Tensile strength is 945 MPa (137 ksi) vs 730 MPa (106 ksi).

Which condition does FabDigit quote by default, Annealed or CD?

HR is the default 4150 condition in the FabDigit quote flow (neither Annealed nor CD). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, 4150 Annealed or 4150-CD?

4150 Annealed. Its machinability rates good (55/100) against fair (50/100) for 4150-CD.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 4150 Annealed and 4150-CD side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.