1015-CD and 1015 Normalized are two conditions of the same steel grade, 1015: CD (cold drawn) versus Normalized. The chemistry is identical, so every difference below comes from the condition. 1015 Normalized is the stronger of the two: tensile strength 424 MPa (61.5 ksi) against 385 MPa (55.8 ksi) for 1015-CD, about 10% more. 1015 Normalized is the more ductile: elongation 37% versus 18% for 1015-CD, and 1015 Normalized is harder (121 HB vs 111 HB).

1015 NormalizedChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

1015-CD vs 1015 Normalized: properties

1015-CD1015 Normalized

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

385 MPa55.8 ksi
424 MPa61.5 ksi

Yield Strength (0.2% offset)

325 MPa47.1 ksi
324 MPa47 ksi

Elongation at Break

18%
37%

Reduction in Area

40%
70%

Shear Strength

270 MPa39.2 ksi
240 MPa34.8 ksi

Fatigue Strength (Endurance Limit)

190 MPa27.6 ksi
205 MPa29.7 ksi

Charpy V-Notch Impact (RT)

85 J62.7 ft·lbf
95 J70.1 ft·lbf

Hardness, Brinell

111 HB
121 HB

Hardness, Rockwell B

65 HRB
69 HRB

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Compressive Strength 190 MPa27.6 ksi

Physical

Density and transition temperatures.

Same in both: Density 7.87 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,495°C2,723 °F · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 51.9 W/m·K30 BTU/hr·ft·°F · Specific Heat Capacity 486 J/kg·K0.12 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.9 µm/m·K6.6 µin/in·°F · Latent Heat of Fusion 247 J/g106 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -30°C-22 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10.8 % IACS · Electrical Resistivity 1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

57 / 100
54 / 100

Machinability Rating (AISI 1212 = 100 %)

65%
62%

Weldability

92 / 100
95 / 100

Formability (cold)

70 / 100
80 / 100

Same in both: Brazeability / Solderability 75 / 100 · Polishability 50 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale1015

1015-CD vs 1015 Normalized — frequently asked

Is 1015 Normalized stronger than 1015-CD?

Yes. 1015 Normalized has a typical tensile strength of 424 MPa (61.5 ksi) against 385 MPa (55.8 ksi) for 1015-CD — about 10% more.

Which condition does FabDigit quote by default, CD or Normalized?

HR is the default 1015 condition in the FabDigit quote flow (neither CD nor Normalized). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose 1015-CD over 1015 Normalized?

Pick 1015 Normalized when strength drives the design, or when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 1015-CD and 1015 Normalized side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.