Stainless Steel S82441-CD vs S82441-SA
Stainless Steel · S82441 temper comparison
S82441-CD and S82441-SA are two conditions of the same stainless steel grade, S82441: CD (cold drawn) versus SA (solution annealed). The chemistry is identical, so every difference below comes from the condition. S82441-CD is the stronger of the two: yield strength 700 MPa (102 ksi) against 550 MPa (79.8 ksi) for S82441-SA, about 27% more; tensile strength follows at 900 MPa (131 ksi) vs 800 MPa (116 ksi). In exchange, S82441-SA is the more ductile: elongation 30% versus 20% for S82441-CD, and S82441-CD is harder (300 HB vs 260 HB).
S82441-CDChoose it when strength drives the design.
S82441-SAChoose it when the part is bent, formed or impact-loaded.
S82441-CD vs S82441-SA: propertiesHow to read these bars
- One bar per material. A full bar is the highest value among all stainless steel grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
How to read these bars
- One bar per material. A full bar is the highest value among all stainless steel grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
Mechanical
Strength, stiffness, ductility and hardness at room temperature.
Tensile Strength (Ultimate)
Yield Strength (0.2% offset)
Elongation at Break
Reduction in Area
Shear Strength
Fatigue Strength (Endurance Limit)
Fracture Toughness (K_IC)
Charpy V-Notch Impact (RT)
Hardness, Brinell
Hardness, Rockwell C
Hardness, Vickers
Same in both: Elastic (Young's) Modulus 200 GPa29 Msi · Shear Modulus 77 GPa11.2 Msi · Bulk Modulus 165 GPa23.9 Msi · Poisson's Ratio 0.3
Physical
Density and transition temperatures.
Same in both: Density 7.7 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,385°C2,525 °F · Liquidus Temperature 1,445°C2,633 °F
Thermal
How each material carries heat and how hot it can run.
Same in both: Thermal Conductivity 15 W/m·K8.7 BTU/hr·ft·°F · Specific Heat Capacity 480 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 13 µm/m·K7.2 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 280°C536 °F · Min Service Temperature -50°C-58 °F
Electrical
Conductivity and insulation.
Same in both: Electrical Conductivity 2.2 % IACS · Electrical Resistivity 8×10⁻⁷ Ω·m31.5 µΩ·in
Chemical & Environmental
Corrosion and environmental resistance (0–100 scores).
Corrosion Resistance
Same in both: Galvanic Potential (seawater, vs SCE) -0.1 V
Manufacturability
FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.
Machinability
Machinability Rating (AISI 1212 = 100 %)
Weldability
Formability (cold)
Same in both: Brazeability / Solderability 40 / 100 · Polishability 75 / 100
Sustainability
Primary-production footprint per kilogram.
Same in both: Embodied Energy (primary production) 55 MJ/kg23,646 BTU/lb · Embodied Carbon (primary production) 5 kg CO₂/kg · Embodied Water 120 L/kg14.4 gal/lb · Typical Recycled Content 60%
Strength versus weight
Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.
S82441-CD vs S82441-SA — frequently asked
Is S82441-CD stronger than S82441-SA?
Yes. S82441-CD has a typical yield strength of 700 MPa (102 ksi) against 550 MPa (79.8 ksi) for S82441-SA — about 27% more. Tensile strength is 900 MPa (131 ksi) vs 800 MPa (116 ksi).
Which condition does FabDigit quote by default, CD or SA?
SA is the default S82441 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.
Which welds better, S82441-CD or S82441-SA?
S82441-SA. Its weldability rates very good (75/100) against very good (70/100) for S82441-CD.
Ready to make it?
Upload a CAD file and FabDigit prices the part in S82441-CD and S82441-SA side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.
Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.