Stainless Steel S82031 Annealed vs S82031 AsWelded
Stainless Steel · S82031 temper comparison
S82031 Annealed and S82031 AsWelded are two conditions of the same stainless steel grade, S82031: Annealed versus AsWelded (as-welded deposit). The chemistry is identical, so every difference below comes from the condition. Both yield at about 610 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (Annealed versus as-welded deposit). S82031 Annealed is the more ductile: elongation 33% versus 25% for S82031 AsWelded.
S82031 AnnealedChoose it when the part is bent, formed or impact-loaded.
S82031 Annealed vs S82031 AsWelded: propertiesHow to read these bars
- One bar per material. A full bar is the highest value among all stainless steel grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
How to read these bars
- One bar per material. A full bar is the highest value among all stainless steel grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
S82031 AnnealedS82031 AsWelded
Mechanical
Strength, stiffness, ductility and hardness at room temperature.
Tensile Strength (Ultimate)
Yield Strength (0.2% offset)
Elongation at Break
Reduction in Area
Compressive Strength
Shear Strength
Fatigue Strength (Endurance Limit)
Fracture Toughness (K_IC)
Charpy V-Notch Impact (RT)
Hardness, Brinell
Hardness, Rockwell B
Hardness, Rockwell C
Hardness, Vickers
Same in both: Elastic (Young's) Modulus 200 GPa29 Msi · Shear Modulus 77 GPa11.2 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3
Physical
Density and transition temperatures.
Same in both: Density 7.8 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,400°C2,552 °F · Liquidus Temperature 1,450°C2,642 °F
Thermal
How each material carries heat and how hot it can run.
Same in both: Thermal Conductivity 15 W/m·K8.7 BTU/hr·ft·°F · Specific Heat Capacity 480 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 13 µm/m·K7.2 µin/in·°F · Latent Heat of Fusion 275 J/g118 BTU/lb · Max Service Temperature (continuous) 300°C572 °F · Min Service Temperature -50°C-58 °F
Electrical
Conductivity and insulation.
Same in both: Electrical Conductivity 2.2 % IACS · Electrical Resistivity 8×10⁻⁷ Ω·m31.5 µΩ·in
Chemical & Environmental
Corrosion and environmental resistance (0–100 scores).
Corrosion Resistance
Same in both: Galvanic Potential (seawater, vs SCE) -0.1 V
Manufacturability
FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.
Machinability
Machinability Rating (AISI 1212 = 100 %)
Formability (cold)
Same in both: Weldability 70 / 100 · Brazeability / Solderability 40 / 100 · Polishability 70 / 100
Sustainability
Primary-production footprint per kilogram.
Same in both: Embodied Energy (primary production) 53 MJ/kg22,786 BTU/lb · Embodied Carbon (primary production) 3.6 kg CO₂/kg · Embodied Water 190 L/kg22.8 gal/lb · Typical Recycled Content 70%
Strength versus weight
Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.
S82031 Annealed vs S82031 AsWelded — frequently asked
What is the difference between S82031 Annealed and S82031 AsWelded?
S82031 Annealed and S82031 AsWelded are two conditions of the same stainless steel grade, S82031: Annealed versus AsWelded (as-welded deposit). The chemistry is identical, so every difference below comes from the condition. Both yield at about 610 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (Annealed versus as-welded deposit).
Which condition does FabDigit quote by default, Annealed or AsWelded?
Annealed is the default S82031 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.
When should I choose S82031 Annealed over S82031 AsWelded?
Pick S82031 Annealed when the part is bent, formed or impact-loaded.
Ready to make it?
Upload a CAD file and FabDigit prices the part in S82031 Annealed and S82031 AsWelded side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.
Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.