FabDigitFabDigit

Stainless Steel S44536-AW vs S44536-SR

Stainless Steel · S44536 temper comparison

S44536-AW and S44536-SR are two conditions of the same stainless steel grade, S44536: AW (as-welded deposit) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. Both yield at about 330 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (as-welded deposit versus stress relieved). S44536-SR is the more ductile: elongation 25% versus 20% for S44536-AW. S44536-SR runs hotter in service (400°C vs 350°C continuous).

S44536-SRChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

S44536-AW vs S44536-SR: properties

S44536-AWS44536-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

490 MPa71.1 ksi
500 MPa72.5 ksi

Elongation at Break

20%
25%

Reduction in Area

45%
57%

Shear Strength

300 MPa43.5 ksi
305 MPa44.2 ksi

Fatigue Strength (Endurance Limit)

210 MPa30.5 ksi
280 MPa40.6 ksi

Fracture Toughness (K_IC)

45 MPa·√m41 ksi·√in
68 MPa·√m61.9 ksi·√in

Charpy V-Notch Impact (RT)

12 J8.9 ft·lbf
28 J20.7 ft·lbf

Hardness, Brinell

178 HB
173 HB

Hardness, Rockwell B

87 HRB
86 HRB

Hardness, Vickers

188 HV
183 HV

Same in both: Elastic (Young's) Modulus 200 GPa29 Msi · Shear Modulus 77 GPa11.2 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Yield Strength (0.2% offset) 330 MPa47.9 ksi · Compressive Strength 330 MPa47.9 ksi

Physical

Density and transition temperatures.

Same in both: Density 7.7 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,450°C2,642 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

350°C662 °F
400°C752 °F

Same in both: Thermal Conductivity 20 W/m·K11.6 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 10 µm/m·K5.6 µin/in·°F · Latent Heat of Fusion 260 J/g112 BTU/lb · Min Service Temperature -30°C-22 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 2.8 % IACS · Electrical Resistivity 6.2×10⁻⁷ Ω·m24.4 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

75 / 100
78 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.1 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

42 / 100
45 / 100

Machinability Rating (AISI 1212 = 100 %)

45%
48%

Weldability

50 / 100
55 / 100

Formability (cold)

40 / 100
56 / 100

Same in both: Brazeability / Solderability 60 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 55 MJ/kg23,646 BTU/lb · Embodied Carbon (primary production) 3.6 kg CO₂/kg · Embodied Water 130 L/kg15.6 gal/lb · Typical Recycled Content 60%

Strength versus weight

Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

3005007001,0001,5002,0007.27.47.67.888.2Density (g/cm³)Yield strength (MPa) — log scaleS44536

S44536-AW vs S44536-SR — frequently asked

What is the difference between S44536-AW and S44536-SR?

S44536-AW and S44536-SR are two conditions of the same stainless steel grade, S44536: AW (as-welded deposit) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. Both yield at about 330 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (as-welded deposit versus stress relieved).

Which condition does FabDigit quote by default, AW or SR?

Annealed is the default S44536 condition in the FabDigit quote flow (neither AW nor SR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, S44536-AW or S44536-SR?

S44536-SR. Its weldability rates good (55/100) against fair (50/100) for S44536-AW.

Ready to make it?

Upload a CAD file and FabDigit prices the part in S44536-AW and S44536-SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.