FabDigitFabDigit

Stainless Steel E307-AW vs E307-SR

Stainless Steel · E307 temper comparison

E307-AW and E307-SR are two conditions of the same stainless steel grade, E307: AW (as-welded deposit) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. Both yield at about 440 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (as-welded deposit versus stress relieved). E307-AW is the more ductile: elongation 38% versus 32% for E307-SR.

E307-AWChoose it when the part is bent, formed or impact-loaded.

E307-AW vs E307-SR: properties

E307-AWE307-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

640 MPa92.8 ksi
655 MPa95 ksi

Yield Strength (0.2% offset)

440 MPa63.8 ksi
460 MPa66.7 ksi

Elongation at Break

38%
32%

Reduction in Area

50%
45%

Compressive Strength

450 MPa65.3 ksi
470 MPa68.2 ksi

Shear Strength

400 MPa58 ksi
410 MPa59.5 ksi

Fatigue Strength (Endurance Limit)

240 MPa34.8 ksi
245 MPa35.5 ksi

Fracture Toughness (K_IC)

130 MPa·√m118 ksi·√in
110 MPa·√m100 ksi·√in

Charpy V-Notch Impact (RT)

60 J44.3 ft·lbf
45 J33.2 ft·lbf

Hardness, Brinell

200 HB
210 HB

Hardness, Rockwell B

92 HRB
94 HRB

Hardness, Vickers

210 HV
220 HV

Same in both: Elastic (Young's) Modulus 193 GPa28 Msi · Shear Modulus 77 GPa11.2 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.28

Physical

Density and transition temperatures.

Same in both: Density 7.9 g/cm³0.29 lb/in³ · Melting Point (Solidus) 1,400°C2,552 °F · Liquidus Temperature 1,450°C2,642 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

15 W/m·K8.7 BTU/hr·ft·°F
15.5 W/m·K9 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 500 J/kg·K0.12 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 17.5 µm/m·K9.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 700°C1,292 °F · Min Service Temperature -120°C-184 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

2.2 % IACS
2.3 % IACS

Electrical Resistivity

8×10⁻⁷ Ω·m31.5 µΩ·in
7.8×10⁻⁷ Ω·m30.7 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

60 / 100
56 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.08 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

32 / 100
30 / 100

Machinability Rating (AISI 1212 = 100 %)

35%
33%

Weldability

92 / 100
88 / 100

Formability (cold)

50 / 100
45 / 100

Same in both: Brazeability / Solderability 55 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 55 MJ/kg23,646 BTU/lb · Embodied Carbon (primary production) 5.5 kg CO₂/kg · Embodied Water 130 L/kg15.6 gal/lb · Typical Recycled Content 55%

Strength versus weight

Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

3005007001,0001,5002,0007.27.47.67.888.2Density (g/cm³)Yield strength (MPa) — log scaleE307

E307-AW vs E307-SR — frequently asked

What is the difference between E307-AW and E307-SR?

E307-AW and E307-SR are two conditions of the same stainless steel grade, E307: AW (as-welded deposit) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. Both yield at about 440 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (as-welded deposit versus stress relieved).

Which condition does FabDigit quote by default, AW or SR?

AW is the default E307 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose E307-AW over E307-SR?

Pick E307-AW when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in E307-AW and E307-SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.