1.4876-CD and 1.4876-SR are two conditions of the same stainless steel grade, 1.4876: CD (cold drawn) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. 1.4876-CD is the stronger of the two: yield strength 480 MPa (69.6 ksi) against 450 MPa (65.3 ksi) for 1.4876-SR, about 7% more. In exchange, 1.4876-SR is the more ductile: elongation 28% versus 25% for 1.4876-CD, and 1.4876-CD is harder (200 HB vs 185 HB). 1.4876-SR runs hotter in service (700°C vs 550°C continuous).

1.4876-CDChoose it when strength drives the design.

1.4876-SRChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

1.4876-CD vs 1.4876-SR: properties

1.4876-CD1.4876-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

690 MPa100 ksi
660 MPa95.7 ksi

Yield Strength (0.2% offset)

480 MPa69.6 ksi
450 MPa65.3 ksi

Elongation at Break

25%
28%

Reduction in Area

50%
45%

Compressive Strength

250 MPa36.3 ksi
450 MPa65.3 ksi

Shear Strength

380 MPa55.1 ksi
445 MPa64.5 ksi

Fatigue Strength (Endurance Limit)

300 MPa43.5 ksi
295 MPa42.8 ksi

Charpy V-Notch Impact (RT)

100 J73.8 ft·lbf
95 J70.1 ft·lbf

Hardness, Brinell

200 HB
185 HB

Hardness, Rockwell B

94 HRB
90 HRB

Hardness, Vickers

215 HV
195 HV

Same in both: Elastic (Young's) Modulus 196 GPa28.4 Msi · Shear Modulus 77 GPa11.2 Msi · Bulk Modulus 190 GPa27.6 Msi · Poisson's Ratio 0.34

Physical

Density and transition temperatures.

Same in both: Density 7.94 g/cm³0.29 lb/in³ · Melting Point (Solidus) 1,357°C2,475 °F · Liquidus Temperature 1,385°C2,525 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

550°C1,022 °F
700°C1,292 °F

Same in both: Thermal Conductivity 11.5 W/m·K6.6 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 14.4 µm/m·K8 µin/in·°F · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 1.7 % IACS · Electrical Resistivity 9.9×10⁻⁷ Ω·m39 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

68 / 100
66 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.15 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Weldability

80 / 100
75 / 100

Same in both: Machinability 35 / 100 · Machinability Rating (AISI 1212 = 100 %) 35% · Formability (cold) 45 / 100 · Brazeability / Solderability 65 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 100 MJ/kg42,992 BTU/lb · Embodied Carbon (primary production) 6.8 kg CO₂/kg · Embodied Water 220 L/kg26.4 gal/lb · Typical Recycled Content 35%

Strength versus weight

Yield strength against density for every stainless steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

3005007001,0001,5002,0007.27.47.67.888.2Density (g/cm³)Yield strength (MPa) — log scale1.4876

1.4876-CD vs 1.4876-SR — frequently asked

Is 1.4876-CD stronger than 1.4876-SR?

Yes. 1.4876-CD has a typical yield strength of 480 MPa (69.6 ksi) against 450 MPa (65.3 ksi) for 1.4876-SR — about 7% more. Tensile strength is 690 MPa (100 ksi) vs 660 MPa (95.7 ksi).

Which condition does FabDigit quote by default, CD or SR?

ANN is the default 1.4876 condition in the FabDigit quote flow (neither CD nor SR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, 1.4876-CD or 1.4876-SR?

1.4876-CD. Its weldability rates very good (80/100) against very good (75/100) for 1.4876-SR.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 1.4876-CD and 1.4876-SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.