Inconel 603-ANN and Inconel 603-AW are two conditions of the same nickel alloy grade, Inconel 603: ANN (annealed) versus AW (as-welded deposit). The chemistry is identical, so every difference below comes from the condition. Inconel 603-AW is the stronger of the two: yield strength 380 MPa (55.1 ksi) against 340 MPa (49.3 ksi) for Inconel 603-ANN, about 12% more. In exchange, Inconel 603-ANN is the more ductile: elongation 45% versus 30% for Inconel 603-AW, and Inconel 603-AW is harder (195 HB vs 180 HB).

Inconel 603-ANNChoose it when the part is bent, formed or impact-loaded.

Inconel 603-AWChoose it when strength drives the design.

Inconel 603-ANN vs Inconel 603-AW: properties

Inconel 603-ANNInconel 603-AW

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

700 MPa102 ksi
660 MPa95.7 ksi

Yield Strength (0.2% offset)

340 MPa49.3 ksi
380 MPa55.1 ksi

Elongation at Break

45%
30%

Reduction in Area

50%
38%

Shear Strength

450 MPa65.3 ksi
425 MPa61.6 ksi

Fatigue Strength (Endurance Limit)

290 MPa42.1 ksi
200 MPa29 ksi

Charpy V-Notch Impact (RT)

100 J73.8 ft·lbf
60 J44.3 ft·lbf

Hardness, Brinell

180 HB
195 HB

Hardness, Rockwell B

88 HRB
91 HRB

Hardness, Vickers

190 HV
205 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 79 GPa11.5 Msi · Bulk Modulus 168 GPa24.4 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.75 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,340°C2,444 °F · Liquidus Temperature 1,400°C2,552 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

1,150°C2,102 °F
1,100°C2,012 °F

Same in both: Thermal Conductivity 11 W/m·K6.4 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 13.4 µm/m·K7.4 µin/in·°F · Latent Heat of Fusion 290 J/g125 BTU/lb · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 1.4 % IACS · Electrical Resistivity 1.25×10⁻⁶ Ω·m49.2 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

80 / 100
74 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.1 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

20 / 100
18 / 100

Machinability Rating (AISI 1212 = 100 %)

12%
10%

Weldability

55 / 100
50 / 100

Formability (cold)

60 / 100
30 / 100

Same in both: Brazeability / Solderability 50 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 160 MJ/kg68,788 BTU/lb · Embodied Carbon (primary production) 13.5 kg CO₂/kg · Embodied Water 400 L/kg47.9 gal/lb · Typical Recycled Content 40%

Strength versus weight

Yield strength against density for every nickel alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0006.577.588.59Density (g/cm³)Yield strength (MPa) — log scaleInconel 603

Inconel 603-ANN vs Inconel 603-AW — frequently asked

Is Inconel 603-AW stronger than Inconel 603-ANN?

Yes. Inconel 603-AW has a typical yield strength of 380 MPa (55.1 ksi) against 340 MPa (49.3 ksi) for Inconel 603-ANN — about 12% more. Tensile strength is 660 MPa (95.7 ksi) vs 700 MPa (102 ksi).

Which condition does FabDigit quote by default, ANN or AW?

ANN is the default Inconel 603 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, Inconel 603-ANN or Inconel 603-AW?

Inconel 603-ANN. Its weldability rates good (55/100) against fair (50/100) for Inconel 603-AW.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Inconel 603-ANN and Inconel 603-AW side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.