WE43B-T5 and WE43B-T6 are two conditions of the same magnesium alloy grade, WE43B: T5 (cooled from hot working and artificially aged) versus T6 (solution heat treated and artificially aged). The chemistry is identical, so every difference below comes from the condition. WE43B-T5 is the stronger of the two: yield strength 205 MPa (29.7 ksi) against 175 MPa (25.4 ksi) for WE43B-T6, about 17% more; tensile strength follows at 310 MPa (45 ksi) vs 255 MPa (37 ksi). WE43B-T5 is the more ductile: elongation 12% versus 8% for WE43B-T6, and WE43B-T5 is harder (90 HB vs 85 HB).

WE43B-T5Choose it when strength drives the design, or when the part is bent, formed or impact-loaded.

WE43B-T5 vs WE43B-T6: properties

WE43B-T5WE43B-T6

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

310 MPa45 ksi
255 MPa37 ksi

Yield Strength (0.2% offset)

205 MPa29.7 ksi
175 MPa25.4 ksi

Elongation at Break

12%
8%

Compressive Strength

190 MPa27.6 ksi
180 MPa26.1 ksi

Shear Strength

170 MPa24.7 ksi
155 MPa22.5 ksi

Fatigue Strength (Endurance Limit)

110 MPa16 ksi
95 MPa13.8 ksi

Fracture Toughness (K_IC)

17 MPa·√m15.5 ksi·√in
15 MPa·√m13.7 ksi·√in

Charpy V-Notch Impact (RT)

6 J4.4 ft·lbf
4 J3 ft·lbf

Hardness, Brinell

90 HB
85 HB

Hardness, Vickers

96 HV
90 HV

Same in both: Elastic (Young's) Modulus 44 GPa6.4 Msi · Shear Modulus 16.5 GPa2.4 Msi · Bulk Modulus 32 GPa4.6 Msi · Poisson's Ratio 0.27

Physical

Density and transition temperatures.

Same in both: Density 1.84 g/cm³0.07 lb/in³ · Melting Point (Solidus) 545°C1,013 °F · Liquidus Temperature 640°C1,184 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

52 W/m·K30 BTU/hr·ft·°F
51 W/m·K29.5 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 966 J/kg·K0.23 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 26.7 µm/m·K14.8 µin/in·°F · Latent Heat of Fusion 350 J/g150 BTU/lb · Max Service Temperature (continuous) 250°C482 °F · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

11.9 % IACS
11.6 % IACS

Electrical Resistivity

1.45×10⁻⁷ Ω·m5.71 µΩ·in
1.48×10⁻⁷ Ω·m5.83 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -1.53 V · Corrosion Resistance 35 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

93 / 100
95 / 100

Machinability Rating (AISI 1212 = 100 %)

290%
300%

Weldability

65 / 100
70 / 100

Formability (cold)

30 / 100
25 / 100

Same in both: Castability 75 / 100 · Brazeability / Solderability 20 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 380 MJ/kg163,371 BTU/lb · Embodied Carbon (primary production) 40 kg CO₂/kg · Embodied Water 500 L/kg59.9 gal/lb · Typical Recycled Content 5%

Strength versus weight

Yield strength against density for every magnesium alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

701001502001.41.51.61.71.8Density (g/cm³)Yield strength (MPa) — log scaleWE43B

WE43B-T5 vs WE43B-T6 — frequently asked

Is WE43B-T5 stronger than WE43B-T6?

Yes. WE43B-T5 has a typical yield strength of 205 MPa (29.7 ksi) against 175 MPa (25.4 ksi) for WE43B-T6 — about 17% more. Tensile strength is 310 MPa (45 ksi) vs 255 MPa (37 ksi).

Which condition does FabDigit quote by default, T5 or T6?

T6 is the default WE43B condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, WE43B-T5 or WE43B-T6?

WE43B-T6. Its weldability rates very good (70/100) against good (65/100) for WE43B-T5.