Duran ANN vs Duran TEMP

Glass · Duran temper comparison

Duran ANN and Duran TEMP are two conditions of the same glass grade, Duran: ANN (annealed) versus TEMP (thermally toughened). The chemistry is identical, so every difference below comes from the condition. Duran TEMP is the stronger of the two: tensile strength 100 MPa (14.5 ksi) against 35 MPa (5.08 ksi) for Duran ANN, about 186% more. Duran ANN runs hotter in service (450°C vs 260°C continuous).

Duran ANNChoose it when the part sees heat.

Duran TEMPChoose it when strength drives the design.

Duran ANN vs Duran TEMP: properties

Duran ANNDuran TEMP

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

35 MPa5.1 ksi
100 MPa14.5 ksi

Flexural Strength

60 MPa8.7 ksi
150 MPa21.8 ksi

Same in both: Elastic (Young's) Modulus 64 GPa9.3 Msi · Shear Modulus 26.7 GPa3.9 Msi · Bulk Modulus 36 GPa5.2 Msi · Poisson's Ratio 0.2 · Elongation at Break 0% · Compressive Strength 1,000 MPa145 ksi · Fracture Toughness (K_IC) 0.75 MPa·√m0.68 ksi·√in · Hardness, Vickers 580 HV · Hardness, Knoop 480 HK · Hardness, Mohs 5.5

Physical

Density and transition temperatures.

Same in both: Density 2.23 g/cm³0.08 lb/in³ · Refractive Index 1.473 · Light Transmission 92% · Porosity 0%

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

450°C842 °F
260°C500 °F

Same in both: Thermal Conductivity 1.2 W/m·K0.69 BTU/hr·ft·°F · Specific Heat Capacity 830 J/kg·K0.2 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 3.3 µm/m·K1.8 µin/in·°F · Min Service Temperature -70°C-94 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Resistivity 1×10¹³ Ω·m3.94×10²⁰ µΩ·in · Dielectric Strength 25 kV/mm635 V/mil · Dielectric Constant (1 MHz) 4.6 · Dissipation Factor (1 MHz) 0.0037 · Volume Resistivity 1×10¹⁵ Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Corrosion Resistance 92 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

10 / 100
3 / 100

Same in both: Polishability 95 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 27 MJ/kg11,608 BTU/lb · Embodied Carbon (primary production) 1.8 kg CO₂/kg · Embodied Water 15 L/kg1.8 gal/lb · Typical Recycled Content 8%

Strength versus weight

Yield strength against density for every glass grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005002.533.5Density (g/cm³)Yield strength (MPa) — log scale

Duran ANN vs Duran TEMP — frequently asked

Is Duran TEMP stronger than Duran ANN?

Yes. Duran TEMP has a typical tensile strength of 100 MPa (14.5 ksi) against 35 MPa (5.08 ksi) for Duran ANN — about 186% more.

Which condition does FabDigit quote by default, ANN or TEMP?

ANN is the default Duran condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, Duran ANN or Duran TEMP?

Duran ANN, by a small margin. Both rate not recommended for machinability — 10/100 against 3/100 for Duran TEMP.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Duran ANN and Duran TEMP side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.