CC766S-GC and CC766S-GM are two conditions of the same copper alloy grade, CC766S: GC (continuously cast bar/tube) versus GM (gravity die cast). The chemistry is identical, so every difference below comes from the condition. CC766S-GC is the stronger of the two: yield strength 185 MPa (26.8 ksi) against 175 MPa (25.4 ksi) for CC766S-GM, about 6% more. CC766S-GC is harder — 62 HRB against 58 HRB for CC766S-GM — which matters for wear surfaces and threads.

CC766S-GCChoose it when strength drives the design, or when surface hardness matters.

CC766S-GC vs CC766S-GM: properties

CC766S-GCCC766S-GM

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

100 GPa14.5 Msi
98 GPa14.2 Msi

Tensile Strength (Ultimate)

450 MPa65.3 ksi
440 MPa63.8 ksi

Yield Strength (0.2% offset)

185 MPa26.8 ksi
175 MPa25.4 ksi

Elongation at Break

15%
16%

Reduction in Area

16%
17%

Shear Strength

305 MPa44.2 ksi
300 MPa43.5 ksi

Fatigue Strength (Endurance Limit)

135 MPa19.6 ksi
125 MPa18.1 ksi

Fracture Toughness (K_IC)

32 MPa·√m29.1 ksi·√in
33 MPa·√m30 ksi·√in

Charpy V-Notch Impact (RT)

19 J14 ft·lbf
21 J15.5 ft·lbf

Hardness, Brinell

110 HB
105 HB

Hardness, Rockwell B

62 HRB
58 HRB

Hardness, Vickers

115 HV
110 HV

Same in both: Shear Modulus 37 GPa5.4 Msi · Bulk Modulus 115 GPa16.7 Msi · Poisson's Ratio 0.34

Physical

Density and transition temperatures.

Same in both: Density 8.35 g/cm³0.3 lb/in³ · Melting Point (Solidus) 885°C1,625 °F · Liquidus Temperature 905°C1,661 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

107 W/m·K61.8 BTU/hr·ft·°F
105 W/m·K60.7 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 380 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 20.5 µm/m·K11.4 µin/in·°F · Latent Heat of Fusion 175 J/g75.2 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -100°C-148 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

22.5 % IACS
22 % IACS

Electrical Resistivity

7.7×10⁻⁸ Ω·m3.03 µΩ·in
7.8×10⁻⁸ Ω·m3.07 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

60 / 100
58 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.25 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

48 / 100
45 / 100

Machinability Rating (AISI 1212 = 100 %)

48%
45%

Same in both: Weldability 35 / 100 · Formability (cold) 28 / 100 · Castability 75 / 100 · Brazeability / Solderability 45 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 55 MJ/kg23,646 BTU/lb · Embodied Carbon (primary production) 3.6 kg CO₂/kg · Embodied Water 250 L/kg30 gal/lb · Typical Recycled Content 70%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleCC766S

CC766S-GC vs CC766S-GM — frequently asked

Is CC766S-GC stronger than CC766S-GM?

Yes. CC766S-GC has a typical yield strength of 185 MPa (26.8 ksi) against 175 MPa (25.4 ksi) for CC766S-GM — about 6% more. Tensile strength is 450 MPa (65.3 ksi) vs 440 MPa (63.8 ksi).

Which condition does FabDigit quote by default, GC or GM?

GS is the default CC766S condition in the FabDigit quote flow (neither GC nor GM). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose CC766S-GC over CC766S-GM?

Pick CC766S-GC when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in CC766S-GC and CC766S-GM side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.