FabDigitFabDigit

Copper Alloy CC755S-GC vs CC755S-GM

Copper Alloy · CC755S temper comparison

CC755S-GC and CC755S-GM are two conditions of the same copper alloy grade, CC755S: GC (continuously cast) versus GM (gravity die cast). The chemistry is identical, so every difference below comes from the condition. Both yield at about 155 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (continuously cast versus gravity die cast). CC755S-GC is harder — 100 HB against 95 HB for CC755S-GM — which matters for wear surfaces and threads.

CC755S-GCChoose it when surface hardness matters.

CC755S-GC vs CC755S-GM: properties

CC755S-GCCC755S-GM

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

98 GPa14.2 Msi
95 GPa13.8 Msi

Tensile Strength (Ultimate)

385 MPa55.8 ksi
370 MPa53.7 ksi

Yield Strength (0.2% offset)

155 MPa22.5 ksi
150 MPa21.8 ksi

Elongation at Break

20%
22%

Compressive Strength

355 MPa51.5 ksi
340 MPa49.3 ksi

Shear Strength

260 MPa37.7 ksi
250 MPa36.3 ksi

Fatigue Strength (Endurance Limit)

110 MPa16 ksi
105 MPa15.2 ksi

Charpy V-Notch Impact (RT)

26 J19.2 ft·lbf
25 J18.4 ft·lbf

Hardness, Brinell

100 HB
95 HB

Hardness, Rockwell B

58 HRB
55 HRB

Hardness, Vickers

105 HV
100 HV

Same in both: Shear Modulus 36 GPa5.2 Msi · Bulk Modulus 115 GPa16.7 Msi · Poisson's Ratio 0.34 · Reduction in Area 22%

Physical

Density and transition temperatures.

Same in both: Density 8.3 g/cm³0.3 lb/in³ · Melting Point (Solidus) 880°C1,616 °F · Liquidus Temperature 900°C1,652 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

112 W/m·K64.7 BTU/hr·ft·°F
110 W/m·K63.6 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 380 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 21 µm/m·K11.7 µin/in·°F · Latent Heat of Fusion 165 J/g70.9 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -100°C-148 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

25 % IACS
24 % IACS

Electrical Resistivity

6.9×10⁻⁸ Ω·m2.72 µΩ·in
7.2×10⁻⁸ Ω·m2.83 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

54 / 100
52 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.26 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

82 / 100
78 / 100

Machinability Rating (AISI 1212 = 100 %)

80%
75%

Formability (cold)

22 / 100
18 / 100

Same in both: Weldability 25 / 100 · Castability 88 / 100 · Brazeability / Solderability 80 / 100 · Polishability 78 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 50 MJ/kg21,496 BTU/lb · Embodied Carbon (primary production) 3.1 kg CO₂/kg · Embodied Water 260 L/kg31.2 gal/lb · Typical Recycled Content 75%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleCC755S

CC755S-GC vs CC755S-GM — frequently asked

What is the difference between CC755S-GC and CC755S-GM?

CC755S-GC and CC755S-GM are two conditions of the same copper alloy grade, CC755S: GC (continuously cast) versus GM (gravity die cast). The chemistry is identical, so every difference below comes from the condition. Both yield at about 155 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (continuously cast versus gravity die cast).

Which condition does FabDigit quote by default, GC or GM?

GM is the default CC755S condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose CC755S-GC over CC755S-GM?

Pick CC755S-GC when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in CC755S-GC and CC755S-GM side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.