FabDigitFabDigit

Copper Alloy CC481K-GC vs CC481K-GM

Copper Alloy · CC481K temper comparison

CC481K-GC and CC481K-GM are two conditions of the same copper alloy grade, CC481K: GC (continuously cast bar/tube) versus GM (permanent (chill) mould cast). The chemistry is identical, so every difference below comes from the condition. CC481K-GC is the stronger of the two: tensile strength 380 MPa (55.1 ksi) against 350 MPa (50.8 ksi) for CC481K-GM, about 9% more. CC481K-GC is the more ductile: elongation 8% versus 4% for CC481K-GM.

CC481K-GCChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

CC481K-GC vs CC481K-GM: properties

CC481K-GCCC481K-GM

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

380 MPa55.1 ksi
350 MPa50.8 ksi

Yield Strength (0.2% offset)

230 MPa33.4 ksi
220 MPa31.9 ksi

Elongation at Break

8%
4%

Compressive Strength

450 MPa65.3 ksi
460 MPa66.7 ksi

Shear Strength

240 MPa34.8 ksi
230 MPa33.4 ksi

Fatigue Strength (Endurance Limit)

130 MPa18.9 ksi
125 MPa18.1 ksi

Charpy V-Notch Impact (RT)

8 J5.9 ft·lbf
6 J4.4 ft·lbf

Hardness, Brinell

105 HB
110 HB

Hardness, Rockwell B

60 HRB
62 HRB

Same in both: Elastic (Young's) Modulus 110 GPa16 Msi · Shear Modulus 41 GPa5.9 Msi · Bulk Modulus 115 GPa16.7 Msi · Poisson's Ratio 0.34

Physical

Density and transition temperatures.

Same in both: Density 8.8 g/cm³0.32 lb/in³ · Melting Point (Solidus) 830°C1,526 °F · Liquidus Temperature 1,000°C1,832 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 47 W/m·K27.2 BTU/hr·ft·°F · Specific Heat Capacity 377 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 18.4 µm/m·K10.2 µin/in·°F · Latent Heat of Fusion 170 J/g73.1 BTU/lb · Max Service Temperature (continuous) 250°C482 °F · Min Service Temperature -200°C-328 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 11 % IACS · Electrical Resistivity 1.57×10⁻⁷ Ω·m6.18 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

65 / 100
66 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.26 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
44 / 100

Machinability Rating (AISI 1212 = 100 %)

30%
29%

Formability (cold)

8 / 100
4 / 100

Same in both: Weldability 20 / 100 · Castability 80 / 100 · Brazeability / Solderability 75 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 70 MJ/kg30,095 BTU/lb · Embodied Carbon (primary production) 4.8 kg CO₂/kg · Embodied Water 320 L/kg38.3 gal/lb · Typical Recycled Content 45%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleCC481K

CC481K-GC vs CC481K-GM — frequently asked

Is CC481K-GC stronger than CC481K-GM?

Yes. CC481K-GC has a typical tensile strength of 380 MPa (55.1 ksi) against 350 MPa (50.8 ksi) for CC481K-GM — about 9% more.

Which condition does FabDigit quote by default, GC or GM?

GC is the default CC481K condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose CC481K-GC over CC481K-GM?

Pick CC481K-GC when strength drives the design, or when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in CC481K-GC and CC481K-GM side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.